Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | |
ND Industries SuperGlue Ethyl 300 General DescriptionA medium to low viscosity cyanoacrylate which is used for bonding plastics and rubber in various combinations.Meets military spec Mil-A-46050C Type II Class II |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | |
ND Industries SuperGlue Ethyl 395 General DescriptionA low viscosity ethyl-based cyanoacrylate that exhibits fast cure speeds on a wide range of common materials such as metals, rubbers, and plastics.Typical Usesloudspeaker componen.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Tensile, (Cured State) |
Palm Labs Adhesives Turbo Fuse Series 130 (100 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 130 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Tensile, (Cured State) |
Palm Labs Adhesives Turbo Fuse Series 150 (500 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 150 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Tensile, (Cured State) |
Palm Labs Adhesives Turbo Fuse Series 160 (1000 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 160 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Tensile, (Cured State) |
Palm Labs Adhesives Turbo Fuse Series 160SI Surface Insensitive (1000 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE 440 SERIES GEL advanced thixotropic formula is designed to polymerize instantly by absorbing surface moisture. The prod.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Tensile, (Cured State) |
Palm Labs Adhesives Turbo Fuse Series 190 (4000 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 190 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Tensile, (Cured State) |
Palm Labs Adhesives Turbo Fuse Series 440 (GEL) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE 280 SERIES SEMI-GEL advanced thixotropic formula is designed to polymerize instantly by absorbing surface moisture. The.. |
|||
Shear Strength | >= 17.2 MPa | >= 2500 psi | |
Master Bond EP45HTMED Epoxy Resists Radiation and Steam Sterilization Description: Master Bond Polymer System EP45HTMED is a two component heat cured epoxy system for high performance structural bonding, sealing, coating and casting. It is especially designed for the .. |
|||
Shear Strength | >= 17.2 MPa | >= 2500 psi | Bond, Al to Al |
Master Bond Supreme 45HTND Toughened Epoxy for Structural Bonding Description: Master Bond Polymer Adhesive SUPREME 45HTND is a two component epoxy adhesive featuring a balance of shear and peel strengths for high performance structural bonding suitable for applic.. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron Ferrobond-LH™ Steel-Filled, Structural Adhesive Putty; High Temperature Liquid Ferrobond-LH™ is Ferrobond-L™ for up to 320° F (160° C) under stress; Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 23 lbs/gal; B: 9.8 lbs/gal; mixin.. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron Metalfix-P™ Aluminum-Filled, Structural Adhesive Putty; Paste Metalfix-P™ is an aluminum-filled, structural adhesive putty. Patch, bond, resurface metal, structural components, patterns, molds, pipes, tanks, sculptures, and appliances. Forms a permanent bond .. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron SS-Bond-P™ Stainless-Steel-Filled, Structural Adhesive Putty; Paste SS-Bond-P™ is a stainless-steel-filled structural adhesive putty. Used where a filler is needed that is as heavy, hard, and wear resistant as iron, but rustproof and more chemical resistant. Common.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Overlap, Steel; ASTM D1002-64 |
3M Scotch-Weld™ CA5 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Higher viscosity, slower setting version of CA4 for filling gaps. Meets CID A-A-3097, Type II, Clas.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Overlap, CRS/CRS |
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Shear Strength | 17.2 MPa | 2500 psi | Overlap, Etched Aluminum, Initial |
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Shear Strength | 17.2 MPa | 2500 psi | Overlap, FR-4 Glass Epoxy |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Overlap, FR-4/FR-4 tested after RT aging |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Overlap, CRS/CRS tested after tap water 1 wk/RT |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 17.2 MPa | 2500 psi | ASTM D1002-94 |
Aremco Aremco-Bond™ 568 High Performance Epoxide Aluminum-Filled, 1:1, Good Bond Strength and High Thermal Conductivity. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron BronzeWeld-P™ Bronze-Filled, Structural Adhesive Putty; Paste BronzeWeld-P™ is a bronze-filled structural adhesive putty. Ideal for statuary, antiques, boats, transportation equipment, vases, railings, metal furniture, metal trim, frames, and instruments. Use.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Tensile Shear Adhesion, on a grit blasted steel |
3M Scotchkote™ RG 501 Urethane Metal Repair Scotchkote Urethane Metal Repair RG 501 has been specifically developed as a rapid curing repair system for rebuilding and repairing equipment requiring good mechanical strength.Product Features:Com.. |
|||
Shear Strength | 17.2 MPa @Temperature -58.0 - -56.0 °C |
2500 psi @Temperature -72.4 - -68.8 °F |
Minimum MIL-A-8623 Type III Requirement |
3M Scotch-Weld™ EC-1386 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M |
|||
Shear Strength | 17.2 MPa | 2500 psi | Overlap, Etched Al, Anti-icing Fluid at RT for 7 days |
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Overlap, Etched Al, JP-4 for 30 days |
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 17.2 MPa @Temperature -55.0 °C |
2500 psi @Temperature -67.0 °F |
Overlap |
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Shear Strength | 17.2 MPa | 2500 psi | Overlap, Etched Aluminum |
3M Scotch-Weld™ DP125 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP125 Translucent is a faster curing version of 3M Scotch-Weld Epoxy Adhesive 2216 Translucent B/A. The worklife and cure time has been reduced from hours and days .. |
|||
Shear Strength | 17.2 MPa @Temperature 21.0 °C |
2500 psi @Temperature 69.8 °F |
Overlap |
3M Scotch-Weld™ DP125 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP125 Translucent is a faster curing version of 3M Scotch-Weld Epoxy Adhesive 2216 Translucent B/A. The worklife and cure time has been reduced from hours and days .. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron Metalfix-L™ Aluminum-Filled, Structural Adhesive Putty; Liquid Metalfix-L™ is a fluid-pourable version of MetalFix-P™. For patterns, molds, prototypes, casting, and all applications where a castable, fluid, MetalFix-P™ is needed. Excellent for tooling. Techn.. |