Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 124 MPa | 18000 psi | ASTM D732 |
Quadrant EPP Duratron® PAI T4503 Compression Molded, Polyamide-imide, Eelectrical Grade (ASTM Product Data Sheet) |
|||
Shear Strength | 124 MPa @Thickness 15.7 mm |
18000 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP504 Glass Fabric Description: Woven glass fabric with high temperature phenolic resin. Good flexural, compressive and impact strengths at elevated temperatures. Capable of continuous operation at 175° C, see note.. |
|||
Shear Strength | 124 MPa @Thickness 15.7 mm |
18000 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP509 Glass Fabric Description: Woven glass fabric, melamine resin laminate. Very hard, flame resistant, machining grade with excellent electrical properties in high humidity conditions. High physical strength and exc.. |
|||
Shear Strength | 124 MPa | 18000 psi | ASTM D732 |
Haysite EHC Glass Reinforced Polyester Sheet, Electrical Grade (GPO1) This IEEE Class F 155ºC high strength material exhibits substantial resistance to cold flow or creep under heat and pressure. Suggested applications include motor slot wedges, washers, brush plat.. |
|||
Shear Strength | 124 MPa | 18000 psi | Typical epoxy composite property; short-beam |
Hexcel® HexTow™ AS4C Carbon Fiber HexTow™ AS4C carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 3,000 (3K), 6,000 (6K), and 12,000 (12K) filament count tows. This fiber has been surface treated.. |
|||
Shear Strength | 124 MPa | 18000 psi | Typical epoxy composite property; short-beam |
Hexcel® HexTow™ AS7 Carbon Fiber HexTow™ AS7 carbon fiber is a continuous, high strength, high strain, PAN based fiber available, in a 12,000 (12K) filament count tow. This fiber has been surface treated and can be sized to improv.. |
|||
Shear Strength | 124 MPa | 18000 psi | Typical epoxy composite property; short-beam |
Hexcel® HexTow™ IM6 Carbon Fiber HexTow™ IM6 carbon fiber is a continuous, high performance, intermediate modulus, PAN based fiber available in 12,000 (12K) filament count tows. The fiber has been surface treated and can be sized .. |
|||
Shear Strength | 124 MPa | 18000 psi | Typical epoxy composite property; short-beam |
Hexcel® HexTow™ IM9 Carbon Fiber HexTow™ IM9 carbon fiber is a continuous, ultrahigh performance, intermediate modulus, PAN based fiber available in 12,000 (12K) filament count tows. The fiber has been surface treated and can be s.. |
|||
Shear Strength | 124 MPa | 18000 psi | Typical epoxy composite property; short-beam |
Hexcel® HexTow™ AS2C Carbon Fiber HexTow™ AS2C carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 3,000 (3K), 6,000 (6K), and 12,000 (12K) filament count tows. This fiber has been surface treated.. |
|||
Shear Strength | 124 MPa | 18000 psi | Typical epoxy composite property; short-beam |
Hexcel® HexTow™ AS4 Carbon Fiber HexTow™ AS4 carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 3,000 (3K), 6,000 (6K), and 12,000 (12K) filament count tows. The fiber has been surface treated a.. |
|||
Shear Strength | 124 MPa | 18000 psi | Typical epoxy composite property; short-beam |
Hexcel® HexTow™ AS4D Carbon Fiber HexTow™ AS4D carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 12,000 (12K) filament count tows. The fiber has been surface treated and can be sized to improve .. |