Hexcel® HexTow™ IM6 Carbon Fiber

Category Carbon , Carbon Fiber
Manufacturer Hexcel
Trade Name HexTow™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexTow™ IM6 Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
HexTow™ IM6 carbon fiber is a continuous, high performance, intermediate modulus, PAN based fiber available in 12,000 (12K) filament count tows. The fiber has been surface treated and can be sized to improve its interlaminar shear properties, handling characteristics, and structural properties. HexTow™ IM6 fiber has shear properties equivalent to those of standard AS type fibers. It is suggested for use in prepregging and filament winding.The unique properties of HexTow™ IM6 fiber, such as lower density (5% less than AS type), higher modulus (20% stiffer than AS type fibers), and good shear strength, allow structural designers to achieve both higher safety margins and lower weights for both stiffness and strength critical applications.Information provided by Hexcel
Physical Properties Metric English Comments
Density 1.76 g/cc
0.0636 lb/in³
Filament Diameter 5.2 µm
5.2 µm
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2760 MPa
400000 psi
Typical epoxy composite property
5700 MPa
827000 psi
Typical fiber property
Elongation at Break 1.9 %
1.9 %
Calculated from tow test data
Tensile Modulus 159 GPa
23100 ksi
Typical epoxy composite property
279 GPa
40500 ksi
Typical fiber property; Chord 6000-1000
Flexural Modulus 145 GPa
21000 ksi
Typical epoxy composite property
Shear Strength 124 MPa
18000 psi
Typical epoxy composite property; short-beam
Component Elements Properties Metric English Comments
Carbon, C 94 %
94 %
Electrical Properties Metric English Comments
Volume Resistivity 0.52 ohm-cm
0.52 ohm-cm
12K
Surface Resistance 0.0014 ohm
0.0014 ohm
12K
Descriptive Properties Value Comments
Approximate Yield (m/g) 2.24
12K
Fiber Volume (%) 62
Tow Cross-Sectional Area (mm2) 0.25
12K
Weight/Length (g/m) 0.446
12K