Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus | 483 MPa | 70000 psi | 0.5 in/min; ASTM D790 |
LyondellBasell Microthene® MP574189 Linear Low Density Polyethylene, Injection Molding Grade ApplicationsMicrothene MP574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items. MP574189 is 16 mesh pow.. |
|||
1% Secant Modulus | 483 MPa | 70000 psi | ASTM D882 |
Total PPR 8650 Polypropylene, Random Copolymer ATOFINA 8650 is a low melting, high ethylene random copolymer with improved color, optics and impact properties. The low melting point of ATOFINA 8650 makes it an excellent heat seal layer for orie.. |