Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM D1922 |
SABIC 218B Linear Low Density Polyethylene for Cast Film Product Description: 218B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM D1922 |
SABIC 518N Linear Low Density Polyethylene for Blown Film Product Description: 548N is a fractional melt index Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resin yield outstanding toug.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM D1922 |
LyondellBasell Alathon® M6010SB High Density Polyethylene, MMW Film Grade Alathon M6010SB is a medium molecular weight high density polyethylene homopolymer for use in blown film applications. Typical applications include those with low WVTR requirements. Regulatory Statu.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM D1922 |
LyondellBasell Petrothene® GA502022 Linear Low Density Polyethylene ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM D1922 |
LyondellBasell Petrothene® GA502024 Linear Low Density Polyethylene ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM D1922 |
Iran Petrochemical (PCC) LL 18XF5 N Linear Low Density Polyethylene LL 18XF5 N is a terpolymer of ethylene, propylene and butene-1 for high film strength applications, especially heavy duty shipping sacks, ice bags, frozen food bags, potato bags, and agriculture fil.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM D1922 |
LyondellBasell Petrothene® GA502023 Linear Low Density Polyethylene ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM D1922 |
Formosa Plastics Formolene® L42009F Film (Butene Grade) LLDPE Extra High Molecular Weight Hexene Copolymer Formolene® L42009F is a general-purpose film grade linear low density made using gas-phase technology. The resin exhibits excellent toughness and streng.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM D1922 |
ExxonMobil Exceed™ 2018CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018CA is a metallocene ethylene-hexene copolymer. The higher melt index makes this polymer ideally suited for blending into LDPE rich films as well as skin layer in coex.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM D1922 |
ExxonMobil LLDPE LL 1001X26 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM D1922 |
ExxonMobil LLDPE LL 1001X31 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM D1922 |
ExxonMobil LLDPE LL 1001X72 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM D1922 |
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM D1922 |
ExxonMobil LLDPE LL 1001X76 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM D1922 |
Dow FLEXOMER™ ETS-9066 NT 7, 0.8 mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9066 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | |
Dow Primacor® 1410 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM-D1922 |
Braskem FG31 LLDPE Blown Film Extrusion Polyethylene Copolymer FG31 is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process. It was developed for blown film extrusion in blends with polyethylene. Films obtained with this pr.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | gF; ASTM D1922 |
Braskem Green PE SLL118/21 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLL118/21 is a LLDPE Butene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties .. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM-D1922 |
Braskem LF118 LLDPE Blown Film Extrusion Polyethylene Copolymer LF118 is a linear low-density polyethylene, copolymer of butene-1, produced by the gas phase process. It is developed for blown film extrusion in blends with polyethylene. Films obtained with this p.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | gF; ASTM D1922 |
Braskem LL118/21 Blown Film Extrusion Linear Low Density Polyethylene Description: LL118/21 is a LLDPE Butene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties a.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM D1922 |
Total Lumicene® mPE M 3410 EP Metallocene Medium Density Film Resin
(Unverified Data**) Polyethylene: Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityHigh StiffnessGood puncture resistanceGood tear strengthGood heat sealing p.. |
|||
Elmendorf Tear Strength TD | 400 - 890 g | 400 - 890 g | Average value: 535 g Grade Count:11 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Blow Molding Grade". Each property range of values reported is .. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | ASTM D1922 |
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made from Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. The.. |
|||
Elmendorf Tear Strength TD | 400 g | 400 g | gF; ASTM D1922 |
Braskem LF0720/20AF Blown Film Extrusion Linear Low Density Polyethylene Description: LF0720/21AF is a LLDPE Butene copolymer produced using Unipol process technology. It shows excellent optical properties associated with good balance of mechanical properties, processing.. |