Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 620 g | 620 g | ASTM D1922 |
Teknor Apex Terraloy™ BP 10000A Thermoplastic Starch + LLDPE Notes: Terraloy™ BP-10001A is a Thermoplastic Starch/LLDPE ready-to-process compound that contains up to 30% of TPS renewable content. This compound is for blown film application. Forms: Pellets A.. |
|||
Elmendorf Tear Strength TD | 620 g | 620 g | Modified rectangular test specimen; ASTM D1922 |
Dow AFFINITY™ PF 1140G Polyolefin Plastomer (POP) AFFINITY™ PF 1140G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed to be used in a variety of demanding applications including form-fill-seal packaging and fre.. |
|||
Elmendorf Tear Strength TD | 620 g | 620 g | ASTM D1922 |
ExxonMobil Escorene® LL-3218 LLDPE/Hexene Premium Cast Stretch Film Resin, 0.8 mil
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3218 have outstanding tensile properties as well as stiffness and toughness. These su.. |