Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 230 g | 230 g | |
Kraton® D1102 + HDPE blend (20/80) Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Elmendorf Tear Strength TD | 230 g | 230 g | ISO 6383-2 |
Topas Advanced Polymers TOPAS® 8007F-04 Cyclic Olefin Copolymer (COC) TOPAS® 8007F-04 is a general purpose film extrusion grade. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and purity for food and.. |
|||
Elmendorf Tear Strength TD | 230 g | 230 g | ASTM D1922 |
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin Product Description: LD 157CW offer good mechanical properties as well as excellent opticals.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesAppl.. |