Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 180 g | 180 g | |
Eastman E6838-997F Polyethylene
(discontinued **) E6838-997F natural is a low density formulation with no slip or antiblock. Outstanding optical properties make this material an excellent choice for calendering and as a clarity filler in co-extrud.. |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
ExxonMobil LD 135.09 Blown Film Resin
(discontinued **) LD 135.09 is a homopolymer film resin with good clarity. Applications include food packaging, light to medium duty bags, and textile packaging.Information provided by ExxonMobil Chemical |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
ExxonMobil LD 145.PX Packaging Resin
(discontinued **) LD 145.PX resin is a homopolymer cast film resin offering good clarity and toughness. Applications include Bread bags and other Food Packaging.Information provided by ExxonMobil Chemical |
|||
Elmendorf Tear Strength TD | 180 - 520 g | 180 - 520 g | Average value: 351 g Grade Count:20 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum.. |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
LyondellBasell Petrothene® GA503027 Linear Low Density Polyethylene (0.5 mil Film) ApplicationsGA 503 is a medium density, butene copolymer LLDPE resin with high draw for stiff, thin blown films. GA 503 contains an antioxidant package to minimize discoloration and eliminate die b.. |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
LyondellBasell Petrothene® NA442051 Low Density Polyethylene ApplicationsPETROTHENE NA 442 is a series of low density/EVA copolymer resins for high impact/high clarity packaging and lamination applications. NA 442 exhibits excellent processability and good b.. |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
LyondellBasell Petrothene® NA963083 Low Density Polyethylene ApplicationsPETROTHENE NA 963 is a series of resins formulated with special antiblock additive and designed for a wide variety of industrial film applications where high impact strength and excellen.. |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
LG Chemical SEETEC BF410 LDPE Characteristics: Good Processability and Excellent Optical PropertiesAdditives: Antiblocking Agent, Slip AgentApplications: Industrial Film & Food PackageCAS No. 9002-88-4Information provided by LG .. |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
LG Chemical SEETEC BF415 LDPE Characteristics: Good Processability and Excellent Optical Properties Applications: Masking filmCAS No. 9002-88-4Information provided by LG Chemical |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
LG Chemical SEETEC BF500 LDPE Characteristics: Good Processability and Good Optical Properties Additives: Antiblocking Agent, Slip AgentApplications: Industrial Film & Food PackageCAS No. 9002-88-4Information provided by LG Chem.. |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
ExxonMobil LD 105.30 Very High Clarity Packaging Film Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
ExxonMobil LDPE LD 105.30 Low Density Polyethylene Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
ExxonMobil LDPE LD 105.BR Low Density Polyethylene Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
ExxonMobil LDPE LD 151BW Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
ExxonMobil LDPE LD 151GZ Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
ExxonMobil LDPE LD 151HR Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
ExxonMobil LDPE LD 364HE Low Density Polyethylene Resin Product Description: LD 364HE is an LDPE, offering a good combination of mechanical, optical and sealing properties.Availability: Africa & Middle East and Europe Additive: Antiblock: 1500 ppmSlip: .. |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
ExxonMobil LDPE LD 380BA Blown Low Density Polyethylene Resin (European Grade) Product Description: LD 380BA offers good toughness and optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Coextrus.. |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM-D1922 |
Braskem FP33 LLDPE Blown Film Extrusion Polyethylene Copolymer The FP33 resin is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process for film extrusion with good mechanical properties. It contains processing aid, slip, and.. |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
3M 6142 Medium Duty Water Activated Paper Tape 3M™ Medium Duty Water Activated Paper Tape 6142 is used for box sealing and other packaging applications. This product has a paper backing and a gummed, high tack, water-activated, modified cornsta.. |
|||
Elmendorf Tear Strength TD | 180 g | 180 g | ASTM D1922 |
ExxonMobil Escorene™ FL 00218 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00218 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 240°C (464°F) may cause resin degradation. Machines should always b.. |