Polymer Property : Tensile Strength, Ultimate = 9000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 34.5 - 62.1 MPa
5000 - 9000 psi
Bulk Molding Compounds BMC 304 Automotive Grade Molding Compound
BMC 304 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 304 can be coated using traditional or electrostatic coati..
Tensile Strength, Ultimate 13.8 - 62.1 MPa
2000 - 9000 psi
Bulk Molding Compounds BMC 606 Mineral Filled, Glass Reinforced Polyester Compound
BMC 606 is a mineral filled, glass reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good moldability, excellent impact strength,..
Tensile Strength, Ultimate 48.3 - 62.1 MPa
7000 - 9000 psi
Bulk Molding Compounds BMC 620X Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 620X molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex..
Tensile Strength, Ultimate 48.3 - 62.1 MPa
7000 - 9000 psi
Bulk Molding Compounds BMC 6241 Glass Fiber Reinforced Compound
BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availabl..
Tensile Strength, Ultimate 48.3 - 62.1 MPa
7000 - 9000 psi
Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound
BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a..
Tensile Strength, Ultimate 48.3 - 62.1 MPa
7000 - 9000 psi
Bulk Molding Compounds BMC 6605A Polyester Molding Compound
Tensile Strength, Ultimate 48.3 - 62.1 MPa
7000 - 9000 psi
Bulk Molding Compounds BMC 8005 Polyester Molding Compound
Tensile Strength, Ultimate 48.3 - 62.1 MPa
7000 - 9000 psi
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound
BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar..
Tensile Strength, Ultimate 20.0 - 62.1 MPa
2900 - 9000 psi
Average value: 36.6 MPa Grade Count:16