Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 440 - 560 MPa
63800 - 81200 psi
Materion Beryllium Copper Alloy 10 Rod and Bar; H (TD04) Temper; up to 76 mm (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 440 - 560 MPa
63800 - 81200 psi
Materion Beryllium Copper Alloy 10 Wire; H (TD04) Temper; 1.3-12.7 mm Diameter (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 440 - 560 MPa
63800 - 81200 psi
Materion Beryllium Copper Alloy 3 Rod and Bar; H (TD04) Temper; up to 76 mm (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 490 - 560 MPa
71100 - 81200 psi
SSAB Tunnplat Aluzink 420A YP High-strength Metal-coated Steel
High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is ..
Tensile Strength, Ultimate 490 - 560 MPa
71100 - 81200 psi
SSAB Tunnplat Dogal 420YP High-strength Metal-coated Steel
High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur..
Tensile Strength, Ultimate 460 - 560 MPa
66700 - 81200 psi
CLAL-MSX NICLAFOR® 1000 TD1 Quenched/Cold Rolled, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Tensile Strength, Ultimate 520 - 560 MPa
75400 - 81200 psi
L direction
ArcelorMittal Save 20-13 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 520 - 560 MPa
75400 - 81200 psi
L direction
ArcelorMittal Save 25-14 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 520 - 560 MPa
75400 - 81200 psi
L direction
ArcelorMittal Save 27-15 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 520 - 560 MPa
75400 - 81200 psi
L direction
ArcelorMittal Save 30-15 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 440 - 560 MPa
63800 - 81200 psi
Materion Beryllium Copper Alloy 3 Tube; H (TD04) Temper; up to 76 mm o.d. (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 440 - 560 MPa
63800 - 81200 psi
Materion Beryllium Copper Alloy 3 Wire; H (TD04) Temper; 1.3-12.7 mm Diameter (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..