Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 26.5 - 45.0 MPa | 3840 - 6530 psi | Average value: 35.7 MPa Grade Count:63 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Tensile Strength, Ultimate | 30.0 - 45.0 MPa @Temperature 60.0 - 90.0 °C |
4350 - 6530 psi @Temperature 140 - 194 °F |
Average value: 37.5 MPa Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Tensile Strength, Ultimate | 20.0 - 45.0 MPa @Temperature 60.0 - 90.0 °C |
2900 - 6530 psi @Temperature 140 - 194 °F |
Average value: 32.5 MPa Grade Count:1 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Tensile Strength, Ultimate | 25.0 - 45.0 MPa | 3630 - 6530 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 1015/0078 PVDF Homopolymer
(discontinued **) Key features of this grade: Plasticized, Offshore, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorina.. |
|||
Tensile Strength, Ultimate | 35.0 - 45.0 MPa | 5080 - 6530 psi | ASTM D638 |
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Tensile Strength, Ultimate | 20.0 - 45.0 MPa @Temperature 60.0 - 150 °C |
2900 - 6530 psi @Temperature 140 - 302 °F |
Average value: 31.3 MPa Grade Count:1 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Tensile Strength, Ultimate | 45.0 - 45.0 MPa @Temperature 60.0 - 60.0 °C |
6530 - 6530 psi @Temperature 140 - 140 °F |
Average value: 45.0 MPa Grade Count:1 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Tensile Strength, Ultimate | 35.0 - 45.0 MPa | 5080 - 6530 psi | ASTM D638 |
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Tensile Strength, Ultimate | 15.2 - 45.0 MPa | 2200 - 6530 psi | Average value: 26.6 MPa Grade Count:55 |
Overview of materials for High Density Polyethylene (HDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim.. |
|||
Tensile Strength, Ultimate | 45.0 - 45.0 MPa @Temperature 136 - 136 °C |
6530 - 6530 psi @Temperature 277 - 277 °F |
Average value: 53.1 MPa Grade Count:1 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |
|||
Tensile Strength, Ultimate | 45.0 - 45.0 MPa @Time 605000 - 605000 sec |
6530 - 6530 psi @Time 168 - 168 hour |
Average value: 53.1 MPa Grade Count:1 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |
|||
Tensile Strength, Ultimate | 27.6 - 45.0 MPa | 4000 - 6530 psi | Average value: 36.4 MPa Grade Count:28 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |
|||
Tensile Strength, Ultimate | 7.00 - 45.0 MPa @Temperature 60.0 - 90.0 °C |
1020 - 6530 psi @Temperature 140 - 194 °F |
Average value: 16.9 MPa Grade Count:4 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Strength, Ultimate | 36.0 - 45.0 MPa | 5220 - 6530 psi | ISO 527 |
BASF Ecoflex® C1200 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2332 is our biodegradable, statistical, aliphatic-aromatic copolyester based on the monomers 1,4-butanediol, adipic acid and terephathalic acid in the polymer chain. E.. |