Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 35.0 - 35.0 MPa @Temperature 60.0 - 60.0 °C |
5080 - 5080 psi @Temperature 140 - 140 °F |
Average value: 35.0 MPa Grade Count:1 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Ultimate | 35.0 - 35.0 MPa @Temperature 32.0 - 32.0 °C |
5080 - 5080 psi @Temperature 89.6 - 89.6 °F |
Average value: 35.0 MPa Grade Count:1 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Tensile Strength, Ultimate | 13.0 - 35.0 MPa | 1890 - 5080 psi | Average value: 24.5 MPa Grade Count:32 |
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum.. |
|||
Tensile Strength, Ultimate | 25.0 - 35.0 MPa | 3630 - 5080 psi | ASTM D638 |
Zeus PFA Tubing PFA, or perfluoroalkoxy, is well recognized for its ability to maintain mechanical integrity in extreme temperatures even when exposed to caustic chemicals. PFA comes in high purity versions that ar.. |
|||
Tensile Strength, Ultimate | 20.0 - 35.0 MPa | 2900 - 5080 psi | ASTM D638 |
Zeus PTFE Tubing Zeus offers a wide range of standard size products and precision custom PTFE Tubing. PTFE Tubing has become the gold standard in industries requiring the ultimate in lubricity, high temperature use,.. |
|||
Tensile Strength, Ultimate | 4.00 - 35.0 MPa | 580 - 5080 psi | ASTM D638 |
Dow Engage® Polyolefin Elastomer Engage® thermoplastic elastomers are ethylene octene copolymers produced via advanced INSITE™ catalyst and process technology, allowing control over polymer structure, properties, and rheology. .. |
|||
Tensile Strength, Ultimate | 15.0 - 35.0 MPa | 2180 - 5080 psi | |
ATG s.r.l. AU-EU Polyurethane Rubber |
|||
Tensile Strength, Ultimate | 27.0 - 35.0 MPa | 3920 - 5080 psi | ISO 527 |
BASF Ecovio® C2224 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |
|||
Tensile Strength, Ultimate | 13.0 - 35.0 MPa | 1890 - 5080 psi | Average value: 23.9 MPa Grade Count:12 |
Overview of materials for Polypropylene with 10% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are .. |