Polymer Property : Tensile Strength, Ultimate = 3630 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.0 - 25.0 MPa

@Temperature 60.0 - 60.0 °C
2900 - 3630 psi

@Temperature 140 - 140 °F
Average value: 22.5 MPa Grade Count:2
Overview of materials for Polystyrene, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr..
Tensile Strength, Ultimate 25.0 - 25.0 MPa

@Temperature 60.0 - 60.0 °C
3630 - 3630 psi

@Temperature 140 - 140 °F
Average value: 25.0 MPa Grade Count:1
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Tensile Strength, Ultimate 12.0 - 25.0 MPa
1740 - 3630 psi
50mm/min; ASTM D638
Micropol Microlink XL Crosslinkable Polyethylene
Characteristics: exceptional toughness, exceptional enviromental stress cracking resistance, outstanding low temperature impact resistance down to -40°C, fully stabilized for outdoor use world wi..
Tensile Strength, Ultimate 7.00 - 25.0 MPa
1020 - 3630 psi
ATG s.r.l. NBR Nitrile-Butadiene Rubber
Tensile Strength, Ultimate 9.00 - 25.0 MPa
1310 - 3630 psi
Average value: 13.0 MPa Grade Count:20
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an..
Tensile Strength, Ultimate 11.0 - 25.0 MPa

@Temperature -30.0 - 70.0 °C
1600 - 3630 psi

@Temperature -22.0 - 158 °F
Average value: 20.3 MPa Grade Count:1
Overview of materials for High Density Polyethylene (HDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim..