Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 68.9 - 207 MPa | 10000 - 30000 psi | Average value: 116 MPa Grade Count:10 |
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Tensile Strength, Ultimate | 121 - 207 MPa | 17500 - 30000 psi | Average value: 158 MPa Grade Count:7 |
Overview of materials for Nylon 11 + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp.. |
|||
Tensile Strength, Ultimate | 138 - 207 MPa | 20000 - 30000 psi | |
Cosmic Plastics CP7311 Epoxy Molding Compound Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 31.0 - 207 MPa | 4500 - 30000 psi | Average value: 144 MPa Grade Count:20 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Tensile Strength, Ultimate | 32.4 - 207 MPa | 4700 - 30000 psi | Average value: 167 MPa Grade Count:84 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |