Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 640 MPa | 92800 psi | Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Ultimate | 640 MPa | 92800 psi | Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4439 Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), and cold rolled strip/sheet forms. |
|||
Tensile Strength, Ultimate | 640 MPa @Temperature 200 °C |
92800 psi @Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 4565 High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Ultimate | 640 MPa @Temperature 300 °C |
92800 psi @Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 4565 High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Ultimate | 640 MPa @Temperature 200 °C |
92800 psi @Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Tensile Strength, Ultimate | 640 - 700 MPa | 92800 - 102000 psi | |
Kennametal Stellite Denertiaâ„¢ N19 Nickel Dental Alloy Denertiaâ„¢ N19 is a low-carbon nickel based porcelain-bonding alloy for the manufacture of dental crowns and bridges.This alloy is Beryllium and Cadmium freeInformation provided by Kennametal St.. |
|||
Tensile Strength, Ultimate | 640 MPa @Temperature 760 °C |
92800 psi @Temperature 1400 °F |
|
Haynes 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Ultimate | 640 MPa | 92800 psi | Rm. 200 HB. |
Assab Steels 760 Machinery Steel ASSAB 760 is an easily machinable carbon steel characterized by: Good machinabilityGood mechanical strengthASSAB 760 is primarily intended to be used in the as-delivered condition. It is only to be .. |
|||
Tensile Strength, Ultimate | 640 MPa | 92800 psi | Typical Annealed |
ATI Allegheny Ludlum AL 600™ Nickel-Base Alloy, UNS N06600 Allegheny Ludlum is a nickel-chromium alloy designed for use from cryogenic to elevated temperatures in the range of 1093 degrees Celsius. AL 600 alloy is non-magnetic and readily weldable. The al.. |