Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 53.9 - 72.0 MPa | 7820 - 10400 psi | Average value: 65.2 MPa Grade Count:19 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Tensile Strength, Ultimate | 53.9 MPa | 7820 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN333HI4 High Impact Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Tensile Strength, Ultimate | 53.9 MPa | 7820 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN173HI3R High Impact Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Tensile Strength, Ultimate | 53.9 MPa | 7820 psi | ASTM D638 |
SK Chemicals SKYPEL M572CR Special Grade Copper Resistance SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Tensile Strength, Ultimate | 53.9 MPa | 7820 psi | ASTM D412 |
SK Chemicals SKYTHANE® X590A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 53.9 MPa | 7820 psi | ASTM D412 |
SK Chemicals SKYTHANE® 590A X series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 53.9 MPa | 7820 psi | ASTM D412 |
Lubrizol Estane® S195A Thermoplastic Polyurethane Type: Estane® S195A is a Shore 95A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, .. |
|||
Tensile Strength, Ultimate | 53.9 MPa | 7820 psi | ASTM D1708 |
Daelim H&L Plavis-G40 DF 40% Graphite Filled Aromatic Polyimide Bearing Direct Formed. Plavis-G-40: Graphite 40 wt% filled, Self lubricating grade with low thermal expansion.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is.. |
|||
Tensile Strength, Ultimate | 53.9 MPa | 7820 psi | DIN 53455; ASTM D638 |
Kolon SPELLOY® KB133HF PC + PBT Alloy Resin