Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 68900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 475 MPa

@Temperature 300 °C
68900 psi

@Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel
Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr..
Tensile Strength, Ultimate 475 MPa
68900 psi
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4713 High Temperature Ferritic Stainless Steel
Does not form brittle phases but should only be exposed to moderately corrosive atmospheres due to low chromium content.Applications: Mostly used in high temperature applications with sulphurous atm..
Tensile Strength, Ultimate 475 MPa

@Temperature 300 °C
68900 psi

@Temperature 572 °F
Annealed prior to test
Special Metals Nickel 200
Commercially pure (99.6%) wrought nickel with good mechanical properties and resistance to a range of corrosive media. Good thermal, electrical, and magnetostrictive properties. Ferromagnetic. Us..
Tensile Strength, Ultimate >= 475 MPa
>= 68900 psi
Guaranteed minimum; long transverse
Alcoa 2324-T39 Aluminum Plate
Alloy 2324-T39 is a higher strength version of alloy 2024-T351 and is a purity controlled composition variant of alloy 2024. It was developed for tension-dominated, fatigue and fracture critical pl..
Copyright © lookpolymers.com All Rights Reserved