Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638-61T |
Rotuba 860H Ethyl Cellulose Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 44.0 MPa @Temperature 120 °C |
6380 psi @Temperature 248 °F |
ISO 527 |
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Global GA-2850 High Density Polyethylene, Blow Molding Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- auto parts, bottles, housewares, drums, containersMeets FDA requirements as listed in food add.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Hannam Chemical Hanalac 710 ABS |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | |
Ineos Styrenics Polystyrene 148G (NAFTA) High heat, easy flow general purpose polystyrene with excellent clarity. Designed for applications requiring a combination of fast processing with good strength and heat resistance.Information prov.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Solvay Specialty Polymers Algoflon® F 5/S Polytetrafluoroethylene (PTFE) Algoflon® F 5/S is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing powder. It is designed for compounds production and in particular it is recommended for use with.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Solvay Specialty Polymers Algoflon® F 7 Polytetrafluoroethylene (PTFE) Algoflon® F 7 is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing. It is designed for normal compression molding and in particular molding of large billets for low .. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Plenco 4300 Phenolic, Granular, Compression Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Elastomer Engineering Elastamide 150 Elastomer Modified RIM Nylon 6 29% crystallinity. Information supplied by Elastomer Engineering. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Tipco Tipcolite® TG 615 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Tipco Tipcolite® TG 617 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | 20 in/min, at max load; ASTM D412 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | |
Williams Advanced Alloys WS179 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Toyobo A2064D Thermoplastic Polyurethane Elastomer, Injection Grade Polycaprolactone type, featuring a good balance of mechanical strength and chemical resistance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Toyobo Pelprene™ S-6001 Polyester TPE Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | 20 in/min, at max load; ASTM D412 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 37 |
Lubrizol ESTANE® GP95AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses:Injection molding partsAvailable in EuropeInformation provided by.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 37 |
Lubrizol ESTANE® GP98AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 98AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Plenco 4002 Phenolic, Granular, Injection Molded PLENCO 04002 is a heat resistant, mineral filled phenolic molding compound offering excellent mechanical strength and dimensional stability at elevated temperatures. UL recognized under component fi.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Toyobo E1095A Thermoplastic Polyurethane Elastomer, Extrusion Grade Polybutyleneadipate type, the most general purpose type of Toyobo Polyurethane; features excellent cost-performance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes,.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 37 |
Lubrizol ESTANE® 58144 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | DIN 53504 |
Lubrizol ESTANE® 58562 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO R527 |
Arkema Group ORGASOL® 3502 D Nat 1 Copolyamide 6/12 Information provided by Arkema Group |
|||
Tensile Strength, Ultimate | 44.0 MPa @Temperature 1093 °C |
6380 psi @Temperature 1999 °F |
ASTM E8 |
ATI Allegheny Ludlum 310S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ATSM D638 |
Ashley Polymers Ashlene® ABS 220 High impact for extrusion. Applications: Extrusion sheet applications including refrigerator door liners and inner box liners, picnic coolers, snow boats, luggage cases, etc.Data provided by the m.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 527B |
Ineos Nova 212 Crystal Polystyrene Low Flow Grade
(discontinued **) Excellent balance of properties; Extrusion and Injection MoldingApplications: Foam insulation, XPS food packaging, Sheet and profile extrusion, CD and DVD jewel boxesProperties were determined on i.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | 20 in/min, at max load; ASTM D412 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 527B |
Ineos Nova 204L Crystal Polystyrene General Purpose Grade
(discontinued **) Fast cycling, Good heat resistance, Good balance of properties and flow characteristics, Extrusion and Injection Molding Applications: General purpose injection molded itemsProperties were determin.. |
|||
Tensile Strength, Ultimate | 44.0 - 55.0 MPa | 6380 - 7980 psi | Average value: 50.6 MPa Grade Count:5 |
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi.. |