Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 33.8 MPa | 4900 psi | ASTM D638-95 |
Multibase Multi-Pro® 0110 X Natural Polypropylene This product is suitable for moldings incorporating high temperature requirements. This material is specially formulated to be resistant to Copper, but is also resistant to most metals.Data provide.. |
|||
Tensile Strength, Ultimate | 33.8 MPa | 4900 psi | ASTM D638-95 |
Multibase Multi-Pro® 1010 T Black 10% Talc Content Polypropylene PPH talc filled compound suitable for containers and wash-tubs requiring elevated stiffness and improved cycle times.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 33.8 MPa | 4900 psi | ASTM D638-95 |
Multibase Multi-Pro® 2005 M 20% Mica Filled Polypropylene Multi-Pro 2005 M is a mica reinforced polypropylene compound with high stiffness and flex strength. Its high heat resistance lends itself to replace engineered plastics at moderate cost.Data provid.. |
|||
Tensile Strength, Ultimate | 33.8 MPa | 4900 psi | ASTM D638 |
Quadrant EPP Proteus® LSG HS PP - Heat Stabilized Polypropylene (ASTM Product Data Sheet) |
|||
Tensile Strength, Ultimate | 33.8 MPa | 4900 psi | ASTM D638 |
Eastman Tenite Butyrate 285A2R30023 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Ultimate | 33.8 MPa | 4900 psi | ASTM D638 |
Eastman Tenite Butyrate 485A2R30016 Natural Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness,.. |
|||
Tensile Strength, Ultimate | 33.8 MPa | 4900 psi | ASTM D638 |
Eastman Tenite Butyrate 530E3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Ultimate | 33.8 MPa | 4900 psi | ASTM D638 |
Eastman Tenite Butyrate 550E4861316 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Ultimate | 33.8 MPa | 4900 psi | ASTM D638 |
Eastman Tenite Butyrate 575E3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Ultimate | 33.8 MPa | 4900 psi | ASTM D638 |
Eastman Tenite Propionate 307A2R30013 Natural, Trsp Cellulose Acetate Propionate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Tensile Strength, Ultimate | 33.8 - 40.2 MPa | 4900 - 5830 psi | UV Postcure; ASTM D638M |
DSM Somos® GP Plus 14122 Somos® GP Plus 14122 is a low-viscosity stereolithography resin with an opaque white appearance. This material mirrors production plastics like ABS and PBT, making it an ideal choice for virtually .. |
|||
Tensile Strength, Ultimate | 33.8 MPa | 4900 psi | ASTM D638 |
Devcon Plastic Steel® Liquid (B) Epoxy General Repair EpoxyComments: Steel-filled liquid epoxy can be cast over models for accurate detail reproduction when making holding fixtures, light-gauge forming dies and molds. Hardens in about a.. |
|||
Tensile Strength, Ultimate | 33.8 MPa | 4900 psi | ASTM D638 |
Adell EQ-16 Homopolymer Polypropylene, 30% Mica Filled Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 33.8 MPa | 4900 psi | |
BCC Products BC 7062-2H Epoxy Casting BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi.. |
|||
Tensile Strength, Ultimate | 33.8 MPa | 4900 psi | ASTM D638 |
Colorite Polymers 3879 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 33.8 MPa | 4900 psi | ASTM D638 |
Eastman Tenite Butyrate 581A3720016 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |