Polymer Property : Tensile Strength, Ultimate = 435 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 3.00 MPa
>= 435 psi
ASTM D412
Multibase Multi-Flex® TPE A 7727 BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tensile Strength, Ultimate 3.00 MPa
435 psi
ASTM D 638
REXtac Rextac® RT 2880 Amorphous Polyalphaolefin (APAO)
Adhesive and Sealant Grade.Description: Butene-1 copolymer and FDA compliantFeatures: Very low softening point and excellent tensile propertiesApplications: Component of hot melt adhesives, sealants..
Tensile Strength, Ultimate 3.00 MPa
435 psi
ASTM D638
ExxonMobil Escorene® LD-783 EVA Copolymer for Specialty Applications  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 33% vinyl acetate copolymerApplications: Soft, injection molded parts; Low modulus applications.
Tensile Strength, Ultimate 3.00 - 177 MPa
435 - 25700 psi
Average value: 114 MPa Grade Count:45
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
Tensile Strength, Ultimate 3.00 - 27.6 MPa
435 - 4000 psi
Average value: 16.6 MPa Grade Count:19
Overview of materials for Polytetrafluoroethylene (PTFE), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Carbon Fiber Filled". Each property range of values reported is minimum ..
Tensile Strength, Ultimate 3.00 - 28.0 MPa
435 - 4060 psi
Average value: 17.6 MPa Grade Count:23
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma..
Tensile Strength, Ultimate 3.00 MPa
435 psi
ASTM D412
Multibase Multi-Flex® TPE 6568 C 1 NATURAL
This product was designed for 2 shot airbag covers with lower tensile strength than currently in use. The moisture content is 1%. The fogging test value is 70% according to ASTM GM 9305P. Multi-F..
Tensile Strength, Ultimate 3.00 MPa
435 psi
In Plane Direction
Cymat A35620SC 030SS Stabilized Aluminum Foam
Description: Cymat A35620SC 030SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.3 g/cm3. The mechanical properties of SAF make it ..
Tensile Strength, Ultimate 3.00 MPa
435 psi
TPE-0153 (ASTM D 412)
Advanced Elastomer Systems Santoprene® 281-45 Thermoplastic Rubber  (discontinued **)
A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be ..
Tensile Strength, Ultimate 3.00 MPa
435 psi
Loctite® Ultra Grey® 5699 Flange Sealant
Silicone GasketingLoctite® Silicone Gasketing materials include unique products with excellent resistance, formulations for high operating temperatures, and UV-curing formulations for cure-in-place..
Tensile Strength, Ultimate 3.00 MPa
435 psi
ASTM D638
ExxonMobil Escorene® UL-7840C EVA Copolymer, Adhesive and Sealant Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 33% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants.