Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 255 MPa | >= 37000 psi | |
PSM Industries PolyAlloys MIM-2200 sintered Low Alloy Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Ultimate | 255 MPa | 37000 psi | |
MTI ThermoStran® PPA-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Tensile Strength, Ultimate | 255 MPa | 37000 psi | |
Williams Advanced Alloys WS363 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 255 - 317 MPa | 37000 - 46000 psi | |
Eagle Brass 110 EPT COPPER, 1/2 Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Tensile Strength, Ultimate | 255 - 276 MPa | 37000 - 40000 psi | |
Eagle Brass 151 ZHC® COPPER, Annealed Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Tensile Strength, Ultimate | 255 - 324 MPa | 37000 - 47000 psi | |
Eagle Brass 210 Gilding Metal, 1/4 Hard CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Tensile Strength, Ultimate | 255 - 317 MPa | 37000 - 46000 psi | |
Eagle Brass 101 OFE COPPER (Certified), 1/2 Hard Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Strength, Ultimate | 255 - 317 MPa | 37000 - 46000 psi | |
Eagle Brass 102 OF COPPER (Non-Certified), 1/2 Hard Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Tensile Strength, Ultimate | 255 MPa | 37000 psi | Worked |
CMW® D582F Silver Graphite Contact Material For electrical contacts; reduced sticking, low voltage DCInformation provided by CMW Inc. |
|||
Tensile Strength, Ultimate | 255 MPa | 37000 psi | annealed |
CMW® ELKONIUM 73 Copper Cadmium Alloy with Au/Ag-Cladding ELKONIUM 73 alloy is a silver, copper, cadmium and gold material marketed by CMW with high electrical and thermal properties. It is designed as an economical rivet type contact for AC applications r.. |
|||
Tensile Strength, Ultimate | 255 MPa | 37000 psi | ATSM D638 |
Ashley Polymers Ashlene® 528L-50LG Nylon 66, 50% Long Glass Fiber Reinforced Long glass fiber reinforced Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than available with conventional glass reinforced resins.Data provi.. |
|||
Tensile Strength, Ultimate | >= 255 MPa | >= 37000 psi | Rm |
ALIMEX 5083 O/H111Aluminum Alloy Rolled Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHAnnealed and slightly strain-hardened |