Tensile Strength, Ultimate 248 MPa
36000 psi
ASTM D638
Techmer ES Electrafil® J-1/CF/30 Nylon 66, 30% Carbon Fiber Reinforced
Carbon Fiber Reinforced
Tensile Strength, Ultimate 248 - 290 MPa
36000 - 42000 psi
Eagle Brass 220 Commercial Bronze, Annealed
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
Tensile Strength, Ultimate 248 MPa
36000 psi
ACMA Test #4
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Tensile Strength, Ultimate 248 MPa
36000 psi
ACMA Test #4
CoorsTek FG-995 Alumina (nom. 98.5% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Tensile Strength, Ultimate 248 MPa
36000 psi
45° stress angle
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic
CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li..
Tensile Strength, Ultimate 248 MPa
36000 psi
90° stress angle
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic
CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li..
Tensile Strength, Ultimate 248 MPa

@Temperature 760 °C
36000 psi

@Temperature 1400 °F
ASTM E8
ATI Allegheny Ludlum 309 Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
Tensile Strength, Ultimate 248 MPa

@Temperature 760 °C
36000 psi

@Temperature 1400 °F
ASTM E8
ATI Allegheny Ludlum 309S Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
Tensile Strength, Ultimate 248 MPa
36000 psi
Parkway Products Thixomolded® AZ91D Magnesium