Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2.07 MPa
300 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8211-65M300 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and ..
Tensile Strength, Ultimate 2.07 MPa
300 psi
Dow Corning 730 SOLVENT RESISTANT SEALANT
Fluorosilicone (solvent resistant) RTV sealantInformation provided by Dow Corning
Tensile Strength, Ultimate 2.07 MPa
300 psi
Cytec EN-12 (Conap) Casting, Potting, and Molding Compound
High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable..
Tensile Strength, Ultimate 2.07 MPa
300 psi
silicone property; ASTM D412
Arlon Thermabond® 99000W008 Silicone Rubber/Fiberglass Laminate
Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Tensile Strength, Ultimate 2.07 MPa
300 psi
silicone property; ASTM D412
Arlon Thermabond® 99000W015 Silicone Rubber/Fiberglass Laminate
Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Tensile Strength, Ultimate 2.07 MPa
300 psi
Dow Corning 3-0105 AUTOMOTIVE SEALANT
One-part RTV, alkoxy cure, designed for automotive powertrain sealing applicationsInformation provided by Dow Corning
Tensile Strength, Ultimate >= 2.07 MPa
>= 300 psi
ASTM C297
Touchstone CFOAM® 20 Structural Carbon Foam
CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins..
Tensile Strength, Ultimate 2.07 MPa
300 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 181-55MED Thermoplastic Elastomer  (discontinued **)
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grades. ..