Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | ASTM D412 |
Multibase Multi-Flex® TPE D 4510 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | >= 15.2 MPa | >= 2200 psi | ASTM D412 |
Multibase Multi-Flex® TPE D 6606 BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | ASTM D638-95 |
Multibase Multi-Pro® 3011 CHI Grey 29% Filler Content Polypropylene Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | |
Freudenberg Simrit Viton® SC1107 CV75WH ETP Excellent resistance to most chemicals. The performance of these products is greater than traditional fluoroelastomers. Avoid use in strong bases or amines. Typical used in wet etch, dry etch, CVD, .. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | |
Kuraray SEPTON® S76 Soft Compound Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its unique isoprene technology. SEPTON® resins are a series of hydrogenated styre.. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | ASTM D638 |
Multibase Multi-Flamâ„¢ 205 HFRI Polypropylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | |
Sylvin Technologies 7056 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | |
Sylvin Technologies 8915-75 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | |
Sylvin Technologies 9915-75 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | |
Sylvin Technologies 9925-90 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | |
Sylvin Technologies 504 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | |
Sylvin Technologies 574 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | |
DuPont Vamac® G Sample Compound Vulcanizate Slab Cure (10 minutes at 177°C) Vulcanizate performance test data can help end-users evaluate the potential fitness of similar compounds for their own applications.Information provided by DuPont. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | Molded property |
Dow DOWLEX™ 2036A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2036A Polyethylene resin is a cast film polymer having improved thermal stability for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a for food .. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | ASTM D412 |
Colorite Polymers CS7533SC Wire and Cable Jacket Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | ASTM D638 |
Colorite Polymers 7088 Non-Phthalate 88 Series Vinyl Compound Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo.. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | |
Colorite Polymers 7511 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | |
Colorite Polymers 7512 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | ASTM D638 |
Colorite Polymers 7772 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | ASTM D638 |
Colorite Polymers 8804 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | ASTM D412 |
Colorite Polymers CS6019GP Non Lead Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | ASTM D412 |
Colorite Polymers CS6033UL Wire and Cable Jacket Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | ASTM D638 |
Buckeye Polymers BP Flex A9505 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | Cured property; ASTM D638 |
Aptek 2201-A/B Fast set urethane adhesive APTEK 2201-A/B is a two component, dark gray, urethane adhesive system displaying excellent adhesion to various plastic, wood, ceramic, and metal substrates. APTEK 2201-A/B is capable of achieving f.. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | cured 2 hours @ 93°C |
Abatron AboCast 8110-2/AboCure 8110-3 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |
|||
Tensile Strength, Ultimate | 15.2 - 45.0 MPa | 2200 - 6530 psi | Average value: 26.6 MPa Grade Count:55 |
Overview of materials for High Density Polyethylene (HDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim.. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 283-40 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Tensile Strength, Ultimate | 15.2 MPa | 2200 psi | |
Sylvin Technologies 6134-80 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.17 MPa | 2200 psi | 500 mm/min; ASTM D412 |
DuPont Performance Polymers Kalrez® 6221 FFKM Perfluoroelastomer Kalrez® parts made from compounds 6221 provide superior chemical resistance and low contamination from extractables in pharmaceutical and food handling applications where FDA compliance is required.. |