Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | ASTM D638-95 |
Multibase Multi-Flex® TPO DEFA 1037 Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® SY-15GB/000 Polystyrene (PS), Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | ASTM D638 |
Huntsman PE 1302 EVA Film Extrusion
(discontinued **) 3% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good low temperature toughness and heat seal characteristics.Applications: Film extrusion: food packaging, general pu.. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | ASTM D4745 |
3M Dyneon™ CC191-HE PTFE, 25% Carbon/Graphite Filled
(discontinued **) Product Form: Black, non-pelletized powder. Applications include bearings, bushings.Data provided by Dyneon. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | ASTM D4745 |
3M Dyneon™ CC607 PTFE 35% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | |
Freudenberg Simrit V60 Standard Fluoroelastomer Excellent resistance to petroleum products and solvents. Very good high-temperature performance. Fluorocarbon elastomers make up the most widely used seals in the semiconductor industry. Avoid polar.. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | |
Sylvin Technologies 8925-70 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | |
Sylvin Technologies 8950-75 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | |
Sylvin Technologies 8980-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | |
Sylvin Technologies 9604-90 LMW Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | |
Sylvin Technologies 9925-70 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | |
Sylvin Technologies 9950-75 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | |
Sylvin Technologies 9960-95 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | |
Sylvin Technologies 9980-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | |
Sylvin Technologies 5104 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | |
Williams Advanced Alloys WS232 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | ISO 527-1/-2 |
DSM Arnitel® VT3104 TPC-ET Extrusion Grade |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | Molded property |
Dow DOWLEX™ 2027A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2027A Polyethylene resin is a higher density polymer for cast film applications with improved stiffness. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2(a) for food contact appli.. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | Molded property |
Dow DOWLEX™ 2047A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2047A Polyethylene resin is a cast film polymer for high performance stretch cling applications. It provides outstanding tear strength, impact strength and toughness. It complies with U.S. .. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | Molded property |
Dow DOWLEX™ 2247A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2247A Polyethylene resin is a cast film polymer for applications requiring outstanding tear strength, impact strength and toughness. This material complies with U.S. FDA Regulation 21 CFR 1.. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | |
Dow LDPE 510I Low Density Polyethylene DOW LDPE 510I resin is a broad molecular weight distribution homopolymer designed to offer excellent impact strength and stress crack resistance with moderate flexibility, for caps/closures, etc. It.. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | |
Dow HDPE 17450N High Density Polyethylene DOW HDPE 17450N resin is a narrow molecular weight distribution copolymer designed to offer low temperature impact strength and gloss with excellent toughness. This resin has good processability ove.. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | |
Colorite Polymers Self Frosting™ 6811SF Vinyl Compound Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi.. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 1070 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | |
Abatron AboCast 7703-21/AboCure 7703-25 (E) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 1080 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | ASTM D638 |
Colorite Polymers 6742A General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | |
Colorite Polymers 6811 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | |
Colorite Polymers 6812 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Tensile Strength, Ultimate | 13.1 MPa | 1900 psi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 2095 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |