Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 11.4 MPa | 1650 psi | ASTM D638 |
Multibase Multi-Flex® TPE D 4112 BLK Ash is 14%. The moisture content is 0.05%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 11.4 MPa | 1650 psi | ASTM D638 |
Chevron Phillips 1400 Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 24200Characteristics: Good Flexibility, Good Flow, Good Warping Resistance, Good Mold Release, Good ESCRApplications:Lids & Closures, C.. |
|||
Tensile Strength, Ultimate | 11.4 MPa | 1650 psi | ASTM D638 |
ExxonMobil Escorene® LD-409 EVA for Low Voltage Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.Applications: Designed to be blended with a suitable masterbatch .. |
|||
Tensile Strength, Ultimate | 11.4 MPa | 1650 psi | |
Freudenberg Simrit V195 Non-Black Compound Specific compounding ingredients can reduce or eliminate the presence of carbon black. These compounds may provide improved resistance to oxidative environments and reactive plasmas. The inorganic p.. |
|||
Tensile Strength, Ultimate | 11.4 MPa | 1650 psi | |
Indium Corp. Indalloy® 3 In-Ag Solder Alloy Has nearly the wettability and low temperature malleability of Indium. Solders silver, fired glass, and ceramics. Large plastic range.Information provided by the manufacturer, Indium Corporation. |
|||
Tensile Strength, Ultimate | 11.4 MPa | 1650 psi | ASTM D3574E |
Mearthane Durethaneâ„¢ M DM-720A Foam Polyurethane MDI backbone: ether.Shore 00 Hardness: 65Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur.. |
|||
Tensile Strength, Ultimate | 11.4 MPa | 1650 psi | |
Sylvin Technologies 9980-90 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 11.4 MPa | 1650 psi | 20 in/min; ASTM D412 |
DuPont Performance Polymers Kalrez® 8475 FFKM Perfluoroelastomer Kalrez® Sahara™ 8475 has been specifically developed to meet the challenging requirements associated with sealing applications in semiconductor thermal processes (i.e., diffusion furnace, LPCVD, R.. |
|||
Tensile Strength, Ultimate | 11.4 MPa | 1650 psi | |
Dow LDPE 779I Low Density Polyethylene DOW LDPE 779I resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent rigidity. Typical applications include caps.. |
|||
Tensile Strength, Ultimate | 11.4 MPa | 1650 psi | ASTM D638 |
Colorite Polymers Elastichem 5011TX-02 Vinyl Compound Description: All components in Elastichem are sanctioned by the U.S. Food & Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulations. For medical use, co.. |
|||
Tensile Strength, Ultimate | 11.4 MPa | 1650 psi | ASTM D638 |
Colorite Polymers 6088 Non-Phthalate 88 Series Vinyl Compound Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo.. |
|||
Tensile Strength, Ultimate | 11.4 MPa | 1650 psi | ASTM D638 |
Westlake EMAC® SP 1257 Ethylene-Methyl Acrylate Copolymer