Material Notes:
Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doorway applications, as well as inside refrigerated area separators. In both cases, low temperatures are likely to be encountered. All components that are used in the manufacturing of these compounds are sanctioned by the U.S. Food and Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulation. Also, because they sanctioned by the US Department of Agriculture, they may be used in meat packaging plants and other food handling areas with no risk of contamination from the entry separators.Information provided by Colorite Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ASTM D2240
Tensile Strength, Ultimate 11.4 MPa
1650 psi
ASTM D638
Elongation at Break 475 %
475 %
ASTM D638
100% Modulus 0.00465 GPa
0.675 ksi
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -65.0 °C
-85.0 °F
ASTM D746
Users viewing this material also viewed the following: