Polymer Property : Tensile Strength, Ultimate = 34.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 15.9 - 34.5 MPa
2310 - 5000 psi
Average value: 28.3 MPa Grade Count:6
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max..
Tensile Strength, Ultimate 24.1 - 34.5 MPa
3500 - 5000 psi
ASTM D638
Premix Premi-Glas® 1201-10 Polyester SMC  (discontinued **)
Premi-Glas® 1201-10 is a 10% glass reinforced thermoset Sheet Molding Compound designed for sinks, shower stall bases and wall applications. Key features and benefits are:Supports ANSI 124.2 and CS..
Tensile Strength, Ultimate 27.6 - 34.5 MPa
4000 - 5000 psi
Bulk Molding Compounds BMC 902 Thermoset Polyester, Soft Flow Encapsulation Grade
BMC 902 is a medium strength, high flow molding compound that meets Ford Specification ESFM3D114- A. BMC 902 has excellent electrical properties and creep resistance. It can be pigmented in a wide r..
Tensile Strength, Ultimate 27.6 - 34.5 MPa
4000 - 5000 psi
Bulk Molding Compounds BMC SLC 1000 Glass Reinforced Polyester
BMC SLC 1000 is a medium strength, low-cost, glass reinforced polyester compound with adjustable shrinkage. It is V-0 flame arc and track resistant. UL® recognized. This material was formerly known..
Tensile Strength, Ultimate 27.6 - 34.5 MPa
4000 - 5000 psi
Bulk Molding Compounds BMC 1410 Electrical Grade
BMC 1410 is a high-strength electrical grade material with excellent flammability resistance. In most applications, this material is competitive with SMC. Equal performance at a lower cost. Normally..
Tensile Strength, Ultimate 20.7 - 34.5 MPa
3000 - 5000 psi
Bulk Molding Compounds BMC 700 Thermoset Polyester, High Arc Quench Electrical Grade
BMC 700 is a general purpose, mineral filled, glass fiber-reinforced polyester compound that was initially designed for molding arc chutes. It has superior arc quench properties. As with all other B..
Tensile Strength, Ultimate 7.85 - 34.5 MPa
1140 - 5000 psi
Average value: 13.2 MPa Grade Count:75
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi..
Tensile Strength, Ultimate 5.00 - 34.5 MPa
725 - 5000 psi
Average value: 20.3 MPa Grade Count:29
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..