Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 7.00 - 24.0 MPa | 1020 - 3480 psi | |
ATG s.r.l. CR Polychloroprene |
|||
Tensile Strength, Ultimate | 12.0 - 24.0 MPa | 1740 - 3480 psi | |
ATG s.r.l. CSM Chlorosulphonated Polyethylene |
|||
Tensile Strength, Ultimate | 8.00 - 24.0 MPa | 1160 - 3480 psi | |
ATG s.r.l. HNBR Hydrogenated Nitrile Butadiene Rubber |