Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 55.2 - 103 MPa | 8000 - 15000 psi | Average value: 74.7 MPa Grade Count:6 |
Overview of materials for PPE/PPO + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Tensile Strength, Ultimate | 53.8 - 103 MPa | 7800 - 15000 psi | Average value: 83.6 MPa Grade Count:25 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Tensile Strength, Ultimate | 48.3 - 103 MPa | 7000 - 15000 psi | Average value: 79.0 MPa Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Tensile Strength, Ultimate | 55.0 - 103 MPa | 7980 - 14900 psi | Average value: 71.5 MPa Grade Count:8 |
Overview of materials for Glass Reinforced, Modified SMA This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Strength, Ultimate | 23.0 - 103 MPa | 3340 - 15000 psi | Average value: 49.2 MPa Grade Count:36 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Tensile Strength, Ultimate | 50.0 - 103 MPa | 7250 - 15000 psi | Average value: 69.7 MPa Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Aramid Fiber Filled". Each property range of values reported is minimu.. |