Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 78.0 - 117 MPa | 11300 - 17000 psi | Average value: 99.0 MPa Grade Count:12 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Tensile Strength, Ultimate | 78.0 MPa | 11300 psi | ASTM D638 |
Plenco 6500 Phenolic, Briquette, Injection Molded PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 .. |
|||
Tensile Strength, Ultimate | 78.0 MPa | 11300 psi | ISO 527-2/1A/5 |
Lubrizol ESTALOC® 59300 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Tensile Strength, Ultimate | 78.0 - 96.0 MPa | 11300 - 13900 psi | |
Dow CYCLOTENE™ 4022-35 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ 4022-35 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |
|||
Tensile Strength, Ultimate | 78.0 - 96.0 MPa | 11300 - 13900 psi | |
Dow CYCLOTENE™ 4024-40 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ 4024-40 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |
|||
Tensile Strength, Ultimate | 78.0 - 96.0 MPa | 11300 - 13900 psi | |
Dow CYCLOTENE™ 4026-46 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ 4026-46 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |
|||
Tensile Strength, Ultimate | 78.0 - 96.0 MPa | 11300 - 13900 psi | |
Dow CYCLOTENE™ XU35075 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ XU35075 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |
|||
Tensile Strength, Ultimate | 78.0 - 96.0 MPa | 11300 - 13900 psi | |
Dow CYCLOTENE™ XU35132 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ XU35132 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |
|||
Tensile Strength, Ultimate | 78.0 - 96.0 MPa | 11300 - 13900 psi | |
Dow CYCLOTENE™ XU35133 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ XU35133 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |
|||
Tensile Strength, Ultimate | 78.0 MPa | 11300 psi | 5 mm/min |
Arkema Group Rilsan® AZM 15 TLD Nylon 12, 15% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLR,16-030,GF15Rigid grade with glass fiber filler (15%) for injection molding.Available color: natural. Light and heat stabilized. Mold-release agent.Rigidity combined wi.. |
|||
Tensile Strength, Ultimate | 78.0 MPa @Temperature 982 °C |
11300 psi @Temperature 1800 °F |
|
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel Characteristics:excellent resistance to general corrosion, excellent resistance to pitting/crevice corrosion, resistant to sensitization, better creep stress-rupture and tensile strength at elevated.. |
|||
Tensile Strength, Ultimate | 78.0 MPa | 11300 psi | ATSM D638 |
Ashley Polymers Ashlene® 73M Nylon 6, Mineral Reinforced A mineral reinforced Nylon 6 with improved impact, excellent dimensional stability and heat resistance.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 78.0 MPa | 11300 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 638 Nylon 6/6, Mineral Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.35% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |