Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 760 MPa | >= 110000 psi | |
MetalTek C86300 High Tensile Manganese Bronze High strength and hardness copper-zinc alloy.Applications: Steel mill nuts, ordnance parts, worm gears.Information provided by MetalTekCast UNS C86300; Cast Grade C86300; Cast ASTM B271, B584, B148;.. |
|||
Tensile Strength, Ultimate | >= 760 MPa | >= 110000 psi | |
MetalTek MTEK 230-B Cast UNS C95500HT Aluminum Bronze Versatile alloy with high strength, good ductility, unusual toughness, plus exceptional wear resistance. Aluminum Bronze heat treated to higher mechanical properties where necessary.Information prov.. |
|||
Tensile Strength, Ultimate | >= 760 MPa | >= 110000 psi | |
MetalTek MTEK CA6NM Cast UNS J91540 Martensitic Stainless Steel "400" series, General corrosion resistant alloys, high strength.Applications: Chemical and food process equipment, jet engine compressor cases and rocket engine parts.Information provided by MetalTe.. |
|||
Tensile Strength, Ultimate | 760 MPa | 110000 psi | |
Haynes Hastelloy® S alloy, weld metal, aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Tensile Strength, Ultimate | 760 MPa | 110000 psi | |
Haynes Hastelloy® S alloy, weld metal, aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Tensile Strength, Ultimate | 760 MPa | 110000 psi | |
Haynes Hastelloy® W alloy, shielded metal arc welds, as-welded Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Tensile Strength, Ultimate | 760 MPa | 110000 psi | |
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Tensile Strength, Ultimate | >= 760 MPa | >= 110000 psi | |
MetalTek IN® 713 UNS N07713 Centri-Vac Nickel Cobalt Based Alloy Information provided by MetalTek |
|||
Tensile Strength, Ultimate | 760 MPa @Temperature 760 °C |
110000 psi @Temperature 1400 °F |
|
Haynes 242® alloy, cold rolled sheet, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Ultimate | 760 MPa @Temperature 650 °C |
110000 psi @Temperature 1200 °F |
|
Haynes 625 alloy, cold rolled and 1050°C mill-annealed sheet Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Tensile Strength, Ultimate | 760 MPa @Temperature 205 °C |
110000 psi @Temperature 401 °F |
|
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Tensile Strength, Ultimate | 760 MPa | 110000 psi | Annealed prior to test |
Special Metals BRIGHTRAY® Alloy C Electrical Resistance Alloy A nickel-chromium electrical-resistance alloy for use at operating temperatures up to 2100°F (1150°C). It contains rare-earth additions for increased oxidation resistance, especially under co.. |
|||
Tensile Strength, Ultimate | 760 MPa @Temperature 650 °C |
110000 psi @Temperature 1200 °F |
Annealed prior to test |
Special Metals INCONEL® Alloy 625 Niobium content includes tantalum. A nickel-chromium-molybdenum alloy with an addition of niobium that acts with the molybdenum to stiffen the alloy's matrix and thereby provide high strength witho.. |
|||
Tensile Strength, Ultimate | 760 MPa | 110000 psi | Typical |
TIMET TIMETAL® 230 Titanium Alloy (Ti-2.5Cu); STA Cold Formable Medium-Strength AlloyFeatures: This binary, age hardening alloy combines the easy formability and weldability of commercially pure titanium with improved mechanical properties, particu.. |
|||
Tensile Strength, Ultimate | 760 MPa | 110000 psi | Typical; Annealed Plate |
ATI Allegheny Ludlum AL 2205™ Duplex Stainless Steel, Plate > 0.1875" Duplex Stainless Steel, UNS S31803 Ferromagnetic. The AL 2205 alloy is a nitrogen-enhanced duplex stainless steel alloy. The nitrogen serves to significantly improved the corrosion resistance of the alloy; especially in the welded c.. |
|||
Tensile Strength, Ultimate | 760 MPa | 110000 psi | Typical |
ATI Allegheny Ludlum AL 400™ Nickel-Base Alloy, Heavily Cold Rolled Sheet and Strip, UNS N04400 Moderately to faintly magnetic at room temperature. Allegheny Ludlum AL 400 alloy is a ductile nickel-copper alloy with resistance to a variety of corrosive conditions. The alloy is most frequentl.. |
|||
Tensile Strength, Ultimate | 760 MPa | 110000 psi | |
ATI Allegheny Ludlum Grade 18 Titanium (UNS R56322) Uses: heat exchangers, industrial components, tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Tensile Strength, Ultimate | 760 MPa | 110000 psi | |
ATI Allegheny Ludlum Grade 9 Titanium (UNS R56320) Uses: heat exchangers, industrial components, tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Tensile Strength, Ultimate | 760 MPa | 110000 psi | |
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367) The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Tensile Strength, Ultimate | 760 MPa | 110000 psi | |
ATI Allvac® AL 6XN® UNS N08367 Specialty Steel Uses: Process equipment, flue-gas scrubber systems, multi-effect evaporators for brines, seawater, pulp & paper liquors.Property values are for samples in the metallurgical condition: 2050°F anneal.. |
|||
Tensile Strength, Ultimate | >= 760 MPa | >= 110000 psi | |
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; A (A) Temper; All Sizes (UNS N03360) Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |
|||
Tensile Strength, Ultimate | 760 MPa | 110000 psi | |
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 50% cold work (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |