Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 552 MPa
80000 psi
Pacific Sintered Materials F-240-S(HT) Steel Powdered Metal
Applications:Medium stressed mechanical componentsEquivalent MPIF Specification: F-0005-60(HT)All information provided by Pacific Sintered Metals.
Tensile Strength, Ultimate 552 MPa
80000 psi
PSM Industries Pacific Sintered Metals Steel F-240-S(HT) Powdered Metal
Medium stressed mechanical components Equivalent MPIF Specification: F-0005-60(HT)Information Provided by Pacific Sintered Metals, a division of PSM Industries
Tensile Strength, Ultimate 552 MPa
80000 psi
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Formed and Deep Draw Quality
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Tensile Strength, Ultimate 552 MPa
80000 psi
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Formed and Deep Draw Quality
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Tensile Strength, Ultimate 552 MPa

@Temperature 649 °C
80100 psi

@Temperature 1200 °F
Kennametal Stellite Deloro® 208 PM after P/M Processing
Adhesive wear test data: cast 0.06 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, s..
Tensile Strength, Ultimate 552 MPa

@Temperature 538 °C
80100 psi

@Temperature 1000 °F
Kennametal Stellite Stellite® 31 PM cast
Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous we..
Tensile Strength, Ultimate 552 - 1240 MPa
80000 - 180000 psi
Meehanite Ductliron® AQS Nodular Graphite Ductile Iron
Type AQS is an air hardening metal possessing high strength, toughness and hardness. It may be fully air quenched throughout casting section after machining to a wide range of strength and hardness..
Tensile Strength, Ultimate 552 - 689 MPa
80000 - 100000 psi
Meehanite Ductliron® SP-80 Nodular Graphite Ductile Iron
Type SP-80 possesses in the as-cast condition more than twice the strength of conventional gray cast iron in combination with exceptional toughness. It has a predominantly pearlitic structure, is r..
Tensile Strength, Ultimate 552 MPa

@Temperature 649 °C
80100 psi

@Temperature 1200 °F
Haynes Hastelloy® C-22® alloy, 12.7-50.8 mm thick bar, solution heat treated
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Ultimate 552 MPa
80000 psi
Universal Wire Works 182 Nickel Alloy Welding Wire
Alloy 182 is used for arc welding Inconel types 600 and 601 to themselves or one to another. Deposited weld metal meets the most stringent radiographic requirements. Alloy 182 dissimilar welding app..
Tensile Strength, Ultimate 552 MPa
80000 psi
Universal Wire Works 320 Stainless Steel Electrode
Universal 320 produces a fully austenitic deposit for welding Carpenter Stainless No. 20Cb-3 (wrought form) or Durimet 20 (cast form) or similar alloys. The 320 alloy was developed to give improved ..
Tensile Strength, Ultimate 552 MPa
80000 psi
Universal Wire Works 80SB-2 Steel Welding Wire
Universal 80SB-2 is a 1/14 chromium 2 molybdenum alloy designed for welding similar composition alloys used primarily in the process industries in steam piping systems and pressure vessels. Weld dep..
Tensile Strength, Ultimate 552 MPa
80000 psi
Universal Wire Works 80SB-2L Steel Welding Wire
Universal 80SB-2L is the same as 80SB-2 with the exception of the carbon content, which is restricted to less than 0.05%.Universal 80SB-2 is a 1/14 chromium 2 molybdenum alloy designed for welding s..
Tensile Strength, Ultimate 552 MPa
80000 psi
Universal Wire Works A Nickel Alloy Welding Wire
Alloy A is used for arc welding various dissimilar combinations of austenitic and ferritic steels and high nickel alloys. For example, when welding Inconel and Incoloy type alloys to carbon steel, s..
Tensile Strength, Ultimate 552 MPa
80000 psi
Universal Wire Works Inconel 62 (AMS 5679) Nickel Alloy Filler Metal
Inconel Filler Metal 62 is a nickel chromium alloy designed for welding nickel base alloy 600 in up to 2" thicknesses using the gas tungsten arc, gas metal arc and submerged arc processes. Filler Me..
Tensile Strength, Ultimate 552 MPa
80000 psi
As Welded
Universal Wire Works Inconel 92 (AMS 5675) Nickel Alloy Filler Metal
Inconel Filler Metal 92 is a nickel base alloy designed especially for gas tungsten arc and gas metal arc welding of dissimilar combinations of high nickel alloys and austenitic and ferritic steels...
Tensile Strength, Ultimate 552 MPa
80000 psi
Tritex TRI-F Blanket Insulation
TRI-F is a unique thermal and acoustic insulation that combines three high temperature fibers in a patented process. The result is a blanket with a service life to 1500°F. By blending fibers of var..
Tensile Strength, Ultimate 552 MPa
80000 psi
Tritex TREO Needled Blanket Insulation
Values and BenefitsBio-soluble fiberEasy to fabricateLow shot contentTypical ApplicationsFurance liningsThermal insulationAcoustic insulationFire protectionHeat shieldsTurbine wrapTypical Industries..
Tensile Strength, Ultimate 552 - 565 MPa
80000 - 82000 psi
Eagle Brass 521 Phosphor Bronzes 8% C, 3/4 Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
Tensile Strength, Ultimate 552 - 689 MPa
80000 - 100000 psi
Eagle Brass 7026 Copper Nickel, Annealed
7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company
Tensile Strength, Ultimate 552 - 689 MPa
80000 - 100000 psi
Eagle Brass 70265 XP175, Annealed
Information provided by Eagle Brass Company
Tensile Strength, Ultimate 552 MPa
80000 psi
Crucible Steel 430F Stainless Steel
Crucible 430F is a low carbon, high chromium ferritic stainless steel, specially developed for solenoid core applications in corrosive environments. The chemistry is closely controlled to develop o..
Tensile Strength, Ultimate 552 MPa
80000 psi
Crucible Steel 446 Chromium Steel
Crucible 446 is a non-hardenable chromium steel which has the highest corrosion and heat resisting properties of the straight chromium steels. This grade is magnetic at all times. Information provi..
Tensile Strength, Ultimate 552 MPa
80000 psi
Crucible Steel 304L Chromium-Nickel Steel
Crucible 304L is a non-hardenable, low carbon austenitic chromium-nickel steel designed for special applications. It is particularly suitable for applications requiring welding operations where it i..
Tensile Strength, Ultimate 552 MPa
80000 psi
cold worked
CMW® ELKONIUM 1 silver, copper, nickel alloy
Alloying copper into silver increases the hardness of the material, and its resistance to mechanical wear and deformation. The electrical and thermal conductivity remain relatively high, thus, the a..
Tensile Strength, Ultimate 552 MPa
80000 psi
cold worked
CMW® ELKONIUM 22 silver, copper alloy
Alloying copper into silver increases the hardness of the material, and its resistance to mechanical wear and deformation. The electrical and thermal conductivity remain relatively high, thus, the a..
Tensile Strength, Ultimate 552 MPa

@Temperature 316 °C
80100 psi

@Temperature 601 °F
Carpenter 20Cb-3® Stainless Steel
Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re..
Tensile Strength, Ultimate 552 MPa
80000 psi
Universal Wire Works 132 Nickel Alloy Welding Wire
Alloy 132 is used for arc welding Inconel type alloy 600 and 601 and stainless alloy 330. Deposited weld metal has excellent high temperature strength and oxidation resistance. The dissimilar weldin..