Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 5.17 MPa | 750 psi | TM R050-36 |
Resinlab® EP1295 Black Medium Viscosity, Halogen Free, Flame Retardant Epoxy Casting Resin Resinlab™ EP1295 Black is a medium viscosity, halogen free, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (.. |
|||
Tensile Strength, Ultimate | 5.17 - 97.0 MPa | 750 - 14100 psi | Average value: 33.7 MPa Grade Count:31 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Tensile Strength, Ultimate | >= 5.17 MPa | >= 750 psi | ASTM D412 |
Multibase Multi-Flex® TPE A 6221 LA BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 5.17 MPa | 750 psi | Dry weak gel; ASTM D412 |
Lubrizol Estane® ALR G2000 Water Absorbent Thermoplastic Polyurethane Type: Estane® ALR G2000 is an aliphatic thermoplastic polyurethane (TPU) resin designed to absorb water and transport moisture.Features: Contains UV additivesAvailable in AmericasInformation Provid.. |
|||
Tensile Strength, Ultimate | 5.17 MPa | 750 psi | Side 2 Silicone Property; ASTM D412 |
Arlon 19646B025 Silicone Rubber/Fiberglass Laminate Side 1:cured silicone rubber; Substrate: 1523 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil Polyethylene |
|||
Tensile Strength, Ultimate | 5.17 MPa | 750 psi | |
BCC Products BC 9040 T Silicone RTV Rubber BC 9040T is a clear, addition/platinum cure, two-component, flowable compound that, regardless of thickness or confinement, cures at room temperature or by application heat. The cured rubber is high.. |
|||
Tensile Strength, Ultimate | 5.17 MPa | 750 psi | ASTM D638 |
Multibase Multi-Flex® A 6221 C TPE Thermoplastic Elastomer Forms: PelletsInformation provided by Multibase |