Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 49.0 MPa | 7100 psi | ASTM D638 |
Nylene® Vexel™ B12U FR Un-reinforced, Flame Retardant PBT Description: Vexel™ B12U FR is an un-reinforced, flame retardant PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources .. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ISO 527 |
LATI LATILUB 73/13-20T Polyoxymethylene Base (POM), 10% Mixed PTFE Self Lubricating Plastic
(Unverified D Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ASTM D638 |
Kolon DIAMAT® EM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ASTM D638 |
Hannam Chemical Hanalac 770 ABS, Extrusion Grade FDA Approved. Excellent mechanical strength, high rigidity, and high impact strength. Good thermoformability. Applications: Refrigerators liners, bathtubs, automobile interiors, portable bags, n.. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN163HI High Impact Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | |
Shinil Chemical SHINCON PETG Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | |
Shinil Chemical SHINSTAT PMMA Electrostatic Control Polymer Injection Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ASTM D638 |
SK Chemicals SKYPEL G182D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ASTM D412 |
SK Chemicals SKYTHANE® 194A L series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ASTM D412 |
SK Chemicals SKYTHANE® L194A Polycaprolactone Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ASTM D412 |
Lubrizol Estane® S198A Thermoplastic Polyurethane Type: Estane® S198A is a Shore 98A, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, .. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ASTM D412 |
Lubrizol Estane® X-595A-11 Thermoplastic Polyurethane Type: Estane® X-595A-11 is a Shore 97A, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Extrusion.Available in AsiaInformation Provided by The Lubr.. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ASTM D638 |
Plenco 08122 Polyester BMC, Compression Molded PLENCO 08122 is a renumber of PlasGlas 10212. PLENCO 08122 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co.. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ASTM D638 |
Plenco 1508 Polyester, Briquette, Transfer Molded PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl.. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ASTM D638 |
Plenco 4349 Phenolic, Granular, Injection Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ASTM D638 |
Plenco 4466 Phenolic, Granular, Injection Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ASTM D638 |
Plenco 7200 Phenolic, Granular, Injection Molded PLENCO 07200 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength, good powder properties and excellent cosmetic properties. UL recognized under component .. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ISO 527-1, 2 |
Polyplastics Duracon® ES-5 Acetal Co-polymer (POM), Conductive, Antistatic DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ASTM D638 |
Elastomer Engineering Elastamide 100 Elastomer Modified RIM Nylon 6 30% crystallinity. Information supplied by Elastomer Engineering. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ASTM D638 |
Tipco Tipcolite® TG 618 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ASTM D638 |
Tipco Tipcolite® TX 311 Phenolic Compound, Wood Flour & Minerals, having Soft Flow & High Strength Soft Flow Phenolic Compound, Reinforced with Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MouldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
I.. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | DIN 53504 |
Lubrizol ESTANE® 58092 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7100 psi | ASTM D412 |
Lubrizol Estane® ALR PC95A Thermoplastic Polyurethane Type: Estane® ALR PC95A is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableAvailable in Americas, Europe, Middle East, Africa, India and Asi.. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ISO 37 |
Lubrizol ESTANE® GP65DE Ester Based Thermoplastic Polyurethane Type: Estane® GP 65DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ASTM D638 |
Plenco 4504 Phenolic, Granular, Compression Molded Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c.. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ISO 527 |
Brueggemann Chemical Nyrim® 1000 (Conditioned) Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc.. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | XY; ASTM D638 |
ALM PA-640-GSL Filled Nylon 12 Prototyping Polymer This carbon fiber/glass sphere filled composite is an easy to process, extremely light weight filled PA 12 material.Improved dimensional stability, recyclability, and increased stiffness.Good Z dire.. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 422 Heavy Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.40% Heavy Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 49.0 MPa | 7110 psi | ASTM D638 |
Plenco 7579 Phenolic, Granular, Injection Molded PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40.. |