Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638-61T |
Rotuba 860H Ethyl Cellulose Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 44.0 MPa @Temperature 120 °C |
6380 psi @Temperature 248 °F |
ISO 527 |
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Global GA-2850 High Density Polyethylene, Blow Molding Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- auto parts, bottles, housewares, drums, containersMeets FDA requirements as listed in food add.. |
|||
Tensile Strength, Ultimate | 44.0 - 130 MPa | 6380 - 18900 psi | Average value: 66.4 MPa Grade Count:15 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Solvay Specialty Polymers Algoflon® F 7 Polytetrafluoroethylene (PTFE) Algoflon® F 7 is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing. It is designed for normal compression molding and in particular molding of large billets for low .. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | 20 in/min, at max load; ASTM D412 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | 20 in/min, at max load; ASTM D412 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Plenco 4300 Phenolic, Granular, Compression Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Plenco 5350 Phenolic, Granular, Injection Molded PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties... |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Tipco Tipcolite® TG 615 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Tipco Tipcolite® TG 617 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Tipco Tipcolite® TX 312 Phenolic Compound, Wood Flour & Minerals having Soft Flow & Lower Density Soft Flow Phenolic Compound, Reinforced with Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MouldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
I.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | 20 in/min, at max load; ASTM D412 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | |
Williams Advanced Alloys WS179 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Toyobo Pelprene™ S-6001 Polyester TPE Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 37 |
Lubrizol ESTANE® GP95AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses:Injection molding partsAvailable in EuropeInformation provided by.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 37 |
Lubrizol ESTANE® GP98AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 98AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Plenco 4002 Phenolic, Granular, Injection Molded PLENCO 04002 is a heat resistant, mineral filled phenolic molding compound offering excellent mechanical strength and dimensional stability at elevated temperatures. UL recognized under component fi.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 37 |
Lubrizol ESTANE® 58144 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | DIN 53504 |
Lubrizol ESTANE® 58562 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO R527 |
Arkema Group ORGASOL® 3502 D Nat 1 Copolyamide 6/12 Information provided by Arkema Group |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ATSM D638 |
Ashley Polymers Ashlene® ABS 220 High impact for extrusion. Applications: Extrusion sheet applications including refrigerator door liners and inner box liners, picnic coolers, snow boats, luggage cases, etc.Data provided by the m.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | 20 in/min, at max load; ASTM D412 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | 20 in/min, at max load; ASTM D412 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ATSM D638 |
Ashley Polymers Ashlene® ABS Resin F-221 High gloss, high impact, extrusion grade.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 527B |
Ineos Nova 204L Crystal Polystyrene General Purpose Grade
(discontinued **) Fast cycling, Good heat resistance, Good balance of properties and flow characteristics, Extrusion and Injection Molding Applications: General purpose injection molded itemsProperties were determin.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 527B |
Ineos Nova 207 Crystal Polystyrene High Heat, High Flow Grade
(discontinued **) Fast cycling, Excellent flow characteristics, Extrusion and Injection Molding Applications: XPS sheet, Foam insulation, CD and DVD jewel boxesProperties were determined on injection molded specimen.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D651 |
Resinoid 2018 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Tensile Strength, Ultimate | 44.0 - 55.0 MPa | 6380 - 7980 psi | Average value: 50.6 MPa Grade Count:5 |
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi.. |