Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 40.7 MPa | 5900 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AS-1000 HI Acrylonitrile Butadiene Styrene (ABS)
(discontinued **) Description/Features:High ImpactPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 40.7 MPa | 5900 psi | |
Indium Corp. Indalloy® 133 Sn-Sb Solder Alloy Higher tensile strength solder than #121. Particular application is joining copper tubing in refrigeration and potable water systems. Has good wettability with good long time sheer strength at 100Â.. |
|||
Tensile Strength, Ultimate | 40.7 MPa | 5900 psi | |
Williams Advanced Alloys WS145 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 40.7 MPa | 5900 psi | |
Williams Advanced Alloys WS303 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 40.7 MPa | 5900 psi | |
Trelleborg Sealing Solutions Turcite® TX Self-Lubricating Thermoplastic Rod Red color. Turcite® TX is engineered to handle moderate load, high speed applications. It exhibits an excellent surface finish when machined. It has a long service life and exceptionally low coe.. |
|||
Tensile Strength, Ultimate | 40.7 MPa | 5900 psi | ASTM D412 |
Lubrizol Estane® ETE 75DT3 Thermoplastic Polyurethane, Easy-to-Extrude Type: Estane® ETE 75DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig.. |
|||
Tensile Strength, Ultimate | 40.7 MPa | 5900 psi | ASTM D638 |
Eastman Tenite Propionate 383A2R30007 Natural, Trsp Cellulose Acetate Propionate Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Tensile Strength, Ultimate | 40.7 MPa | 5900 psi | ASTM D638 |
Eastman Tenite Propionate 360E0096907 Natural, Trsp Cellulose Acetate Propionate Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness, .. |
|||
Tensile Strength, Ultimate | 40.7 MPa | 5900 psi | ASTM D638 |
Eastman Tenite Acetate 109E3V46022 Natural, Trsp Cellulose Acetate
(discontinued **) Plasticizer 25%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.2% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Ultimate | 40.7 - 130 MPa | 5900 - 18900 psi | Average value: 66.1 MPa Grade Count:38 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |