Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 35.2 MPa | 5100 psi | ASTM D638 |
Multibase Nylex™ 2185 FR Polyamide + PP Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodFlame RetardantForms:PelletsProcessing Methods:Injection MoldingUses: Electric.. |
|||
Tensile Strength, Ultimate | 35.2 MPa | 5110 psi | ASTM Data |
Styron Magnum™ 555 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 35.2 MPa | 5110 psi | ASTM Data |
Styron Magnum™ 585 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 35.2 MPa | 5110 psi | ASTM Data |
Styron Magnum™ 9015 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 35.2 MPa | 5100 psi | |
Williams Advanced Alloys WS292 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 35.2 MPa | 5110 psi | ASTM Data |
Dow Prevail® 3050 ABS + Polyurethane PREVAIL® 3050 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used .. |
|||
Tensile Strength, Ultimate | 35.2 MPa | 5110 psi | ASTM D638 |
Adell EA-14 Homopolymer Polypropylene, 20% Talc Filled Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 35.2 MPa | 5100 psi | ASTM D412 |
AdvanSource Biomaterials ChronoThane™ P Thermoplastic Polyurethane Elastomer AdvanSource Biomaterials Corporation manufactures and markets aromatic-based ChronoThane™ P. Some characteristics that have made it attractive to medical device manufacturers include low coefficien.. |
|||
Tensile Strength, Ultimate | 35.2 MPa | 5100 psi | after optimum cure |
Armstrong A-12-T Epoxy Adhesive Provides the same basic properties as A-12, but in thixotropic, non-sag, easily-brushable paste form. An ideal material for use where adhesive flow during cure cannot be tolerated. A-12-T meets t.. |
|||
Tensile Strength, Ultimate | 35.2 MPa | 5110 psi | ASTM D638 |
Adell EQ-14 Homopolymer Polypropylene, 20% Mica Filled Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 35.2 MPa | 5110 psi | ASTM D638-95 |
Multibase Multi-ABS 2925 FR Flame Retardant ABS Data provided by Multibase. |