Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
Pacific Sintered Materials FCC-216-P High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
PSM Industries Pacific Sintered Metals Nickel Steel FN-255-S Powdered Metal Good impact resistant mechanical components, Good hardenability Equivalent MPIF Specification: FN-0205-25Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Ultimate | >= 345 MPa | >= 50000 psi | |
PSM Industries PolyAlloys MIM-430L sintered Stainless Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Ultimate | >= 345 MPa | >= 50000 psi | |
Kobe Steel KS60AKOT Titanium alloy with low alloying elements, ASTM Gr. 33, Annealed Nominal Composition: Ti-0.4 Ni-0.015 Pd-0.025 Ru-0.14 Cr Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant... |
|||
Tensile Strength, Ultimate | >= 345 MPa | >= 50000 psi | |
Kobe Steel KSTI-1.5AL Alpha Titanium Alloy, Annealed Nominal Composition: Ti-1.5 Al Applications: Exhaust systems.Features:Heat resistant. Information provided by Kobe Steel |
|||
Tensile Strength, Ultimate | >= 345 MPa | >= 50000 psi | |
Kobe Steel Titanium alloy with low alloying elements, ASTM Gr. 7, Annealed Nominal Composition: Ti-0.15 Pd Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant. Information provided by .. |
|||
Tensile Strength, Ultimate | 345 - 517 MPa | 50000 - 75000 psi | |
Materion ToughMet® T3 CA ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Tensile Strength, Ultimate | 345 - 448 MPa | 50000 - 65000 psi | |
Meehanite AQ Flake Graphite Cast Iron Type AQ is a wear and abrasion resisting iron that is readily machinable as-cast but may be "air-hardened" after machining with minimum risk of cracking or distortion. Type AQ is easily heat treate.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
Meehanite GA-50 Flake Graphite Cast Iron Type GA-50 combines high strength, toughness, wear resistance and damping capacity with excellent machinability. Responds well to heat treatment, local and surface hardening.General Meehanite infor.. |
|||
Tensile Strength, Ultimate | >= 345 MPa | >= 50000 psi | |
MetalTek AGMA CL B UNS C91700 Gear Bronze Copper-tin alloy with high tensile, yield and compressive strength as well as wear resistance.Applications: Worm gears, steel mill nutsInformation provided by MetalTekCast UNS C91700; Cast Grade C91.. |
|||
Tensile Strength, Ultimate | >= 345 MPa | >= 50000 psi | |
MetalTek MTEK CZ-100 Cast UNS N02100 Severe Corrosion and Heat Resistant Alloy Strong, tough and resistant to a wide range of industrial chemicals.Applications: Process equipment; food, pharmaceutical and chemical.Information provided by MetalTek |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | ASTM D638 |
Glastic Laminates/Shapes MTS Grade MTS Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | Annealed |
Special Metals Nickel 205 Wrought nickel similar to Nickel 200 but with compositional adjustments to enhance performance in electrical and electronic applications. Ferromagnetic. Used for the anodes and grids of electronic.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | Annealed |
Special Metals Nickel 270 A high-purity grade of nickel made by powder metallurgy. It has a low base hardness and high ductility. Its extreme purity is useful for components of hydrogen thyratrons. It is also used for ele.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
Universal Wire Works 187 Copper-Nickel Alloy Welding Wire Alloy 187 is used for arc welding of wrought or cast 70/30, 80/20, and 90/10 copper nickel alloys to themselves or to each other. Alloy 187 can be used for welding the clad side of copper-nickel cla.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
Universal Wire Works Commercially Pure (AMS 4951) Titanium Alloy Filler Metal Universal commercially pure titanium is extremely versatile for applications requiring high temperature resistance together with resistance to many chemical reagents. Commercially pure (cp) titanium.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | Typical |
TIMET TIMETAL® 35A CP Titanium (ASTM Grade 1) Commercially Pure Titanium.Industry Specifications: Germany Engineering: 3.7025. Germany Aerospace: 3.7024. France: T-35. UK Aerospace Specification: BS TA. 1.Features: The mechanical properties.. |
|||
Tensile Strength, Ultimate | 345 - 469 MPa | 50000 - 68000 psi | |
Eagle Brass 735 Nickel Silver 18%, Annealed 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | Premium Casting |
CMW® 3 Copper Alloy CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | cold worked |
CMW® D50F Silver Nickel Alloy CMW® D50F can be fabricated into wire, rod and strip; however, the headability of CMW® D50F is limited to a narrow range. It is used for main contacts in circuit breakers and switching devices whe.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | cold worked |
CMW® ELKONIUM 23 silver, copper alloy Alloying copper into silver increases the hardness of the material, and its resistance to mechanical wear and deformation. The electrical and thermal conductivity remain relatively high, thus, the a.. |
|||
Tensile Strength, Ultimate | 345 - 400 MPa | 50000 - 58000 psi | |
Eagle Brass 101 OFE COPPER (Certified), Spring Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | cold worked |
CMW® ELKONIUM 70 gold based alloy Pure gold has complete resistance to atmospheric tarnish and oxidation. It does not contribute to polymer formations like platinum and palladium alloys. Wrought gold metal is very soft and prone to .. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
Ametek P316L P/M Stainless Steel, Sintered from 6.30 g/cc Green Density P316L offers a very high degree of corrosion protection for a standard P/M stainless steel grade. It provides excellent strength at extremely high temperatures. Key materials benefits of P316L inclu.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
ATI Allegheny Ludlum Grade 1 Titanium (UNS R50250) Uses: CPI equipment, industrial components, plate frame heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
ATI Allegheny Ludlum Grade 17 Titanium (UNS R52252) Uses: CPI equipment, industrial components, plate frame heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
ATI Allvac® Grade 7 UNS R52400 Titanium Alloy Uses: Industrial components, CPI equipment, heat exchangers, pressure vessels, fittings, tubings.Property values are for samples in the metallurgical condition: 1300°F anneal.Information provided b.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | Typical |
Aleris Weldural Aluminum Alloy, 500 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
ATI Allvac® 40, Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal Data provided by Allvac.Applications: Airframe components, cryogenic vessels, heat exchangers, CPI equipment, condenser tubing, pickling baskets. |