Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | X, Y direction; ASTM D638 |
Rogers Corporation RT/duroid® 6202 High Frequency Laminate Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric.. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ISO 527-2 |
NOVA Chemicals DYLARK® 378 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | |
Chevron Phillips 7108T LLDPE Sheeting Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 214, A 35307Applications:Cast Geomembrane Applications, Sanitary Landfill Liners, Waste Water Reservoir Containm.. |
|||
Tensile Strength, Ultimate | 30.0 MPa @Temperature 60.0 °C |
4350 psi @Temperature 140 °F |
ISO 527 |
LATI LATAN 3E71 Polyoxymethylene Copolymer (POM) with Elastomer
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Tensile Strength, Ultimate | 30.0 - 50.0 MPa | 4350 - 7250 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 21508 PVDF Copolymer
(discontinued **) Key features of this grade: High Elongation, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® P.. |
|||
Tensile Strength, Ultimate | 30.0 - 62.0 MPa | 4350 - 8990 psi | Average value: 48.7 MPa Grade Count:21 |
Overview of materials for Phenolic, Novolac, Impact Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum .. |
|||
Tensile Strength, Ultimate | 30.0 - 160 MPa @Temperature -40.0 - 150 °C |
4350 - 23200 psi @Temperature -40.0 - 302 °F |
Average value: 66.6 MPa Grade Count:7 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Tensile Strength, Ultimate | 30.0 - 215 MPa | 4350 - 31200 psi | Average value: 149 MPa Grade Count:581 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Tensile Strength, Ultimate | 30.0 - 299 MPa | 4350 - 43400 psi | Average value: 219 MPa Grade Count:91 |
Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Tensile Strength, Ultimate | 30.0 - 159 MPa | 4350 - 23100 psi | Average value: 87.4 MPa Grade Count:22 |
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi.. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | |
Kuraray HYBRAR® PH7 Polypropylene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Strength, Ultimate | 30.0 MPa @Temperature 1205 °C |
4350 psi @Temperature 2201 °F |
|
Haynes 214® alloy, cold rolled annealed sheet 2.0-3.2 mm thick Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Tensile Strength, Ultimate | 30.0 MPa @Temperature 1204 °C |
4350 psi @Temperature 2199 °F |
|
Haynes HR-160® alloy, hot rolled and solution annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | DIN 53504 |
Lubrizol ESTANE® T5090 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | DIN 53504 |
Lubrizol ESTANE® X4928 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ISO 527-1 |
Chengdu Polyster FH605 Thermoplastic Polyether-ester Elastomer (TPEE) Blend of H605 and self-made flame retardant material. Flame retardant, high tear resistance. Applications requiring flame retardancy, such as wires, cables and optical fiber.Information provided by .. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ISO 527-1 |
Chengdu Polyster H5550B Thermoplastic Polyether-ester Elastomer (TPEE) Low modulus molding and extrusion grade. Contains color-stable antioxidants. Good balance of low and high temperature properties. Excellent flex-fatigue resistance. Excellent creep resistance. CVJ b.. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ISO 527-1 |
Dow BETAMATE™ 1045 Epoxy BETAMATE™ 1045 is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excellent.. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ASTM D412 |
BASF Elastollan® 1175AW Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Tensile Strength, Ultimate | 30.0 - 50.0 MPa | 4350 - 7250 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 20810 PVDF Copolymer
(discontinued **) Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ASTM D638 |
Toyobo Pelprene™ S-1001 Polyester TPE Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block.. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | DIN 53504 |
Lubrizol ESTANE® 54630 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ISO 37 |
Lubrizol ESTANE® 58141 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 30.0 - 35.9 MPa | 4350 - 5210 psi | Average value: 33.9 MPa Grade Count:3 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |
|||
Tensile Strength, Ultimate | 30.0 MPa @Temperature 900 °C |
4350 psi @Temperature 1650 °F |
|
Resistalloy International Fecralloy™ 134 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small labora.. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | |
Kraton® D1102 + PP blend (50/50) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |