Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 17.2 MPa | 2490 psi | ASTM D638 |
Multibase Multi-Flex® TPE D 4310 Multi-Flex® D 4310 Natural was designed to replace Himont's CA 53 G material. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | >= 17.2 MPa | >= 2490 psi | ASTM D412 |
Multibase Multi-Flex® TPE G 7890 BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | ASTM D638 |
Multibase Multi-Pro® 2513 C Whirlpool White Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | TM R050-36 |
Resinlab® EP1285HD-12 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2490 psi | ASTM D638-95 |
Multibase Multi-Flex® TPO D-6206 This TPO product was developed for facia applications exhibiting adhesion for current automotive paint systems.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2490 psi | ASTM D638 |
Chevron Phillips 4538B LDPE Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 05200Characteristics: Good Flexibility, Moderate Flow, Moderate Warping Resistance, Good Mold Release, Excellent ESCRApplications:Perso.. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2490 psi | |
Freudenberg Simrit V176 Standard Fluoroelastomer Excellent resistance to petroleum products and solvents. Very good high-temperature performance. Fluorocarbon elastomers make up the most widely used seals in the semiconductor industry. Avoid polar.. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | |
Sylvin Technologies 6151-89 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | |
Sylvin Technologies 8950-90 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | |
Sylvin Technologies 9604-85 Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | |
Sylvin Technologies 50423 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | |
Sylvin Technologies 5117-82 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | |
Sylvin Technologies 6034-85 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | |
Sylvin Technologies 6034-85 UV PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | ASTM D882 |
Total PPR Z9450 Random Copolymer Heat Sealable Grade ATOFINA Z9450 is a low melting, high ethylene random copolymer with improved color, optics and impact properties. The very low melting point of ATOFINA Z9450 makes it an excellent heat seal layer f.. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | ASTM D638 |
CPC - Vycom FLAMETEC™ CP7-D Flame Retardant Polypropylene Flametec™ CP7-D is a proprietary designation for a flame retardant polypropylene formulation. CP7-D represent our version of polypropylene sheet whose flame retardant characteristics meet or exceed.. |
|||
Tensile Strength, Ultimate | 17.2 MPa @Temperature 1040 °C |
2500 psi @Temperature 1900 °F |
|
Crucible Steel 446 Chromium Steel Crucible 446 is a non-hardenable chromium steel which has the highest corrosion and heat resisting properties of the straight chromium steels. This grade is magnetic at all times. Information provi.. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | ASTM D412 |
Colorite Polymers CS6037GP Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | ASTM D412 |
Colorite Polymers CS9039UL Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | ASTM D412 |
Colorite Polymers Weatherflex™ CS1532WX (NTL01P) Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | ASTM D638 |
Colorite Polymers 7502 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | ASTM D638 |
Colorite Polymers 8334 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | ASTM D638 |
Colorite Polymers 8533 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | |
Dymax 930 Coil Terminating, Tamper proofing and Structural Electronic Bonder High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 930 Coil Terminating, Tamper proofing and Structural Electronic BonderHigh strength, superior bonds to steel, alumin.. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | ASTM D412 |
Advanced Polymer Alloys DURACRYN 8080 NC Thermoplastic Rubber Information provided by Advanced Polymer Alloys |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | |
AIM 100In Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2490 psi | Cured 7 min at 177°C and Post Cured 16 hr at 232°C |
DuPont Performance Polymers VTR 8525 (GBLT-S) GFLT-600 Formulation
(discontinued **) FormulationViton® GFLT 600 |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | |
Sylvin Technologies 5120 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 17.2 MPa | 2500 psi | Bond strength to glass |
Dymax Light Weld® 429 High Clarity Glass Bonding Adhesive Glass Bonding in SecondsDescriptionDymax Light Weld® 400 Series adhesives form high-clarity, invisible bonds between glass and other substrates in seconds. In addition to many structural glass bond.. |