Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 5.00 - 6.00 J | 3.69 - 4.43 ft-lb | Average value: 5.33 J Grade Count:3 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Dart Drop, Total Energy | 4.00 - 6.00 J | 2.95 - 4.43 ft-lb | Average value: 5.33 J Grade Count:3 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |