Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CM5820 PC+ABS (Asia Pacific) Cycoloy CM5820 resin is a Mineral Filled Non-FR PC+ABS blend with high impact, high modulus, good chemical resistance & improved surface aesthetic, designed for hand help device chassis that require.. |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS Cycoloy Medium Heat Plating Grade for Automotive |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impact |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Asia Pacific) UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® BFL2000 PC (Asia Pacific) Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors. |
|||
Dart Drop, Total Energy | 55.0 J | 40.6 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® IR1810 PC (Europe-Africa-Middle East) IR1810 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® LUX9130T PC COPOLYMER (Asia Pacific) LUX9130T Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm / 5VA rating at 6.0mm and is U.. |
|||
Dart Drop, Total Energy | 55.0 J | 40.6 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® PC2200 PC (Europe-Africa-Middle East) PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Dart Drop, Total Energy | 55.0 J | 40.6 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® PC2200R PC (Asia Pacific) PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dart Drop, Total Energy | 55.0 J | 40.6 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® PC2200R PC (Europe-Africa-Middle East) PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dart Drop, Total Energy | 55.0 J | 40.6 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® VR1820 PC (Europe-Africa-Middle East) VR1820 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS (Europe-Africa-Middle East) Cycoloy Medium Heat Plating Grade for Automotive |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Asia Pacific) High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impact |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® BFL2000U PC Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig.. |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® BFL2000U PC (Asia Pacific) Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig.. |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® BFL2000U PC (Europe-Africa-Middle East) Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig.. |
|||
Dart Drop, Total Energy | 55.0 J | 40.6 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics PC2200 PC (Asia Pacific) PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Dart Drop, Total Energy | 55.0 J | 40.6 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics PC2200 PC (Europe-Africa-Middle East) PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Dart Drop, Total Energy | 55.0 J | 40.6 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics PC2200R PC (Asia Pacific) PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dart Drop, Total Energy | 55.0 J | 40.6 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics PC2203R PC (Asia Pacific) PC2203R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dart Drop, Total Energy | 55.0 J | 40.6 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics PC2800 PC (Europe-Africa-Middle East) PC2800 resin is a high flow (MFR = 28 at 300°C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release... |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East) VALOX 412 is 20% glass reinforced PBT injection moulding resin. Applications: Spotlights, appliance housings and handles. |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East) Super high flow FR PBT grade with 15% Glass reinforced |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® X5601WX PBT + PC + PET Impact modified PBT+PC+PET, Heat aging improved Xenoy |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
2.2 m/sec; ASTM D3763 |
Styron PULSEâ„¢ 2000 EZ PC/ABS Engineering Resin Overview: PULSE 2000 Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can wi.. |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL 731 PPE+HIPS (Asia Pacific) PPE+PS, HDT 125 |
|||
Dart Drop, Total Energy | 55.0 J @Temperature 23.0 °C |
40.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CY4000M PC+ABS (Asia Pacific) Cycoloy* CY4000M resin is an injection moldable, flame retardant PC/ABS blend free of chlorinated or brominated flame resistant additives. Cycoloy CY4000M resin has excellent flow and balanced impac.. |