Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 51.0 J | 37.6 ft-lb | SABIC Method |
SABIC Innovative Plastics Lexan® FL903 PC Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance, excellent impact, flexural strength/rigidity. UV-stabilized. |
|||
Dart Drop, Total Energy | 51.0 J | 37.6 ft-lb | SABIC Method |
SABIC Innovative Plastics Lexan® FL900 PC (Asia Pacific) Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance excellent impact, flexural strength/rigidity. UL94 V-1 at .157"" (3.99 mm). |
|||
Dart Drop, Total Energy | 51.0 J @Temperature 23.0 °C |
37.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FXM123R PC (Asia Pacific) FXM123R is a Lexan PC grade in Metallic or Pearlescent effects, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package .. |
|||
Dart Drop, Total Energy | 51.0 J @Temperature 23.0 °C |
37.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FXM123R PC (Europe-Africa-Middle East) FXM123R is a Lexan PC grade in Metallic or Pearlescent effects, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package .. |
|||
Dart Drop, Total Energy | 51.0 J | 37.6 ft-lb | SABIC Method |
SABIC Innovative Plastics Lexan® FL900 PC Lexan* resin FL900 is a Br- & Cl-free flame retardant grade that can be foamed for weight reductions. UL-94 V1 listed at 3.9mm together with good stiffness, heat, creep and impact performance make i.. |
|||
Dart Drop, Total Energy | 51.0 J | 37.6 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL SE1X PPE+PS (Asia Pacific) PPO+PS. Improved productivity and reliability. Nonchlorinated, nonbrominated flame retardant. 244F HDT. |
|||
Dart Drop, Total Energy | 51.0 J | 37.6 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRILOY D20001 PC (Asia Pacific) LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant. |
|||
Dart Drop, Total Energy | 51.0 J | 37.6 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 POLYPHENYLENESULFONE (Asia Pacific) LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral. |
|||
Dart Drop, Total Energy | 51.0 J | 37.6 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 PPS LNP* THERMOCOMP* 9X04488 is a compound based on PPS resin containing Mineral. |
|||
Dart Drop, Total Energy | 51.0 J | 37.6 ft-lb | 0.1 in thick, 15 mph; ASTM D1822 |
Styron CALIBREâ„¢ IM 401-18 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dart Drop, Total Energy | 51.0 J | 37.6 ft-lb | 0.125 in, 8000 ipm; ASTM D3763 |
Styron EMERGEâ„¢ 4410-18 MFR Polycarbonate EMERGEâ„¢ PC 4410-18 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l.. |
|||
Dart Drop, Total Energy | 51.0 J | 37.6 ft-lb | Peak Energy; ASTM D3763 |
Diamond Polymers DIAMALOY PC 1812 Impact Modified Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |