Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1200-15 Polycarbonate Resin Description: LUPOY PC 1200-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1201-10 Polycarbonate Resin Description: LUPOY PC 1201-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1201-15 Polycarbonate Resin Description: LUPOY PC 1201-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1300-15 Polycarbonate Resin Description: LUPOY PC 1300-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1301-10 Polycarbonate Resin Description: LUPOY PC 1301-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1301-12 Polycarbonate Resin Description: LUPOY PC 1301-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1301V-10 Polycarbonate Resin Description: LUPOY PC 1301V-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 3010-22 Polycarbonate Resin Description: LUPOY PC 3010-22 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 3030-10 Polycarbonate Resin Description: LUPOY PC 3030-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 3030-15 Polycarbonate Resin Description: LUPOY PC 3030-15 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy NF1007F 10R Polycarbonate Resin Description: LUPOY NF 1007F10R, eco-friendly UL94 V0/3.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar.. |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy NF1009F 15 Polycarbonate Resin Description: LUPOY NF 1009F15, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpare.. |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1300-10 Polycarbonate Resin Description: LUPOY PC 1300-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1303-10 Polycarbonate Resin Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1303AH-10 Polycarbonate Resin Description: LUPOY PC 1303AH-10 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and .. |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1303AH-15 Polycarbonate Resin Description: LUPOY PC 1303AH-15 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and .. |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 3010-30 Polycarbonate Resin Description: LUPOY PC 3010-30 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203 m/min; ASTM D1822 |
Styron CALIBREâ„¢ 201-10 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dart Drop, Total Energy | 87.0 J | 64.2 ft-lb | 8000 ipm; ASTM D3763 |
Styron CALIBREâ„¢ 2061-15 Polycarbonate CALIBREâ„¢ 2061-15 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and.. |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203 m/min; ASTM D1822 |
Styron CALIBREâ„¢ 301-10 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203 m/min; ASTM D1822 |
Styron CALIBREâ„¢ 301-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dart Drop, Total Energy | 87.0 J | 64.2 ft-lb | ASTM D3763 |
Styron CALIBREâ„¢ 303V-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300V-10 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products are avai.. |
|||
Dart Drop, Total Energy | 87.0 J | 64.2 ft-lb | 8000 ipm; ASTM D3763 |
Styron EMERGEâ„¢ 4310-10 Polycarbonate EMERGEâ„¢ PC 4310-10 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq.. |
|||
Dart Drop, Total Energy | 87.0 J | 64.2 ft-lb | 8000 ipm; ASTM D3763 |
Styron EMERGEâ„¢ 4330-10 Polycarbonate EMERGEâ„¢ PC 4330-10 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information.. |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203 m/min; ASTM D1822 |
Styron CALIBREâ„¢ 201-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dart Drop, Total Energy | 87.0 J | 64.2 ft-lb | 3.39 m/sec; ASTM D3763 |
Styron CALIBREâ„¢ 302-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203 m/min; ASTM D1822 |
Styron CALIBREâ„¢ 303-10 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dart Drop, Total Energy | 87.0 J @Thickness 3.20 mm |
64.2 ft-lb @Thickness 0.126 in |
203 m/min; ASTM D1822 |
Styron CALIBREâ„¢ 303-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dart Drop, Total Energy | 87.0 J | 64.2 ft-lb | 8000 ipm; ASTM D3763 |
Styron EMERGEâ„¢ 4310-15 Polycarbonate EMERGEâ„¢ PC 4310-15 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq.. |