Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.701 kN/m @Temperature 24.0 °C |
4.00 pli @Temperature 75.2 °F |
Aluminum T-Peel; ASTM D1876 |
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |
|||
Peel Strength | 0.701 kN/m @Temperature 82.0 °C |
4.00 pli @Temperature 180 °F |
Aluminum T-Peel; ASTM D1876 |
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |
|||
Peel Strength | 0.701 kN/m @Temperature -55.0 °C |
4.00 pli @Temperature -67.0 °F |
Aluminum T-Peel; ASTM D1876 |
3M Scotch-Weld™ 183 B/A Tan Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |
|||
Peel Strength | 0.701 kN/m @Temperature 24.0 °C |
4.00 pli @Temperature 75.2 °F |
Aluminum T-Peel; ASTM D1876 |
3M Scotch-Weld™ 183 B/A Tan Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |
|||
Peel Strength | 0.701 kN/m @Temperature 82.0 °C |
4.00 pli @Temperature 180 °F |
Aluminum T-Peel; ASTM D1876 |
3M Scotch-Weld™ 183 B/A Tan Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |
|||
Peel Strength | 0.701 kN/m @Temperature 24.0 °C |
4.00 pli @Temperature 75.2 °F |
Aluminum T-Peel; ASTM D1876 |
3M Scotch-Weld™ 183 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flowable product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent e.. |
|||
Peel Strength | 0.701 kN/m @Temperature 82.0 °C |
4.00 pli @Temperature 180 °F |
Aluminum T-Peel; ASTM D1876 |
3M Scotch-Weld™ 183 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flowable product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent e.. |
|||
Peel Strength | 0.701 kN/m @Temperature 14.0 °C, Time 1.81e+6 sec |
4.00 pli @Temperature 57.2 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 847 Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |
|||
Peel Strength | 0.701 kN/m @Temperature 14.0 °C, Time 1.81e+6 sec |
4.00 pli @Temperature 57.2 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 847-H Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsHigh viscosity grade adhesive for many brush or spray applications.Quick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |
|||
Peel Strength | 0.701 kN/m @Temperature 66.0 °C |
4.00 pli @Temperature 151 °F |
180° |
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro.. |
|||
Peel Strength | 0.701 kN/m @Temperature 23.0 °C |
4.00 pli @Temperature 73.4 °F |
180° T-Peel, Nitrile/CRS |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Peel Strength | 0.701 kN/m @Temperature 107 °C |
4.00 pli @Temperature 225 °F |
Adhesion on Aluminum; ASTM D3330 |
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Peel Strength | 0.701 kN/m @Temperature 107 °C |
4.00 pli @Temperature 225 °F |
Adhesion on Aluminum; ASTM D3330 |
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Peel Strength | 0.701 kN/m @Temperature 150 °C |
4.00 pli @Temperature 302 °F |
Adhesion on Aluminum; ASTM D3330 |
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Peel Strength | 0.701 kN/m @Temperature 150 °C |
4.00 pli @Temperature 302 °F |
Adhesion on Aluminum; ASTM D3330 |
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Peel Strength | 0.701 kN/m @Temperature 82.0 °C |
4.00 pli @Temperature 180 °F |
180°, Canvas/Steel |
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive Features: A light colored, fast drying adhesiveExcellent resistance to aromatic fuels, water and oilUsed to bond many types of plastic films including ABS, cellulose acetate, and PVCInformation prov.. |
|||
Peel Strength | 0.701 kN/m @Temperature 14.0 °C, Time 1.81e+6 sec |
4.00 pli @Temperature 57.2 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 847-L Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |
|||
Peel Strength | 0.701 kN/m @Temperature 66.0 °C, Time 1.81e+6 sec |
4.00 pli @Temperature 151 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1870 Industrial Adhesive Features: A fast drying, highly flexible adhesive with very long tack range and good water resistanceFor bonding fabrics and most other lightweight materials with little or no tendency to stain or b.. |