Polymer Property : Peel Strength = 5.26 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 5.26 kN/m

@Temperature 91.0 °C
30.0 pli

@Temperature 196 °F
resistance to glass; ASTM D3167
Huntsman KRYSTALFLEX® PE 501 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
Peel Strength 5.26 kN/m

@Temperature 24.0 °C,
Time 432000 sec
30.0 pli

@Temperature 75.2 °F,
Time 120 hour
canvas/canvas
3M Fastbond™ 30-NF Contact Adhesive
3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M
Peel Strength 5.26 kN/m

@Temperature 24.0 °C,
Time 1.81e+6 sec
30.0 pli

@Temperature 75.2 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1099-L Nitrile High Performance Plastic Adhesives
Features: It is a low viscosity grade for spray application.Fast dryingProvides strong, flexible bonds.Resists weathering, water, fuels, oil and plasticizers.Bonds vinyl extrusions and sheeting. (Ma..
Peel Strength 5.26 kN/m

@Temperature 24.0 °C,
Time 1.21e+6 sec
30.0 pli

@Temperature 75.2 °F,
Time 336 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1300 Neoprene High Performance Rubber Gasket Adhesives
3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre..
Peel Strength 5.26 kN/m

@Temperature 24.0 °C,
Time 1.81e+6 sec
30.0 pli

@Temperature 75.2 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive
Features: Alight colored, high strength adhesive with a long tack rangeExcellent water, oil and grease resistanceBonds neoprene, natural, reclaim SB-R and butyl rubber to most substrates.Information..
Peel Strength 5.26 kN/m

@Temperature 24.0 °C,
Time 1.81e+6 sec
30.0 pli

@Temperature 75.2 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 4491 Nitrile Industrial Adhesive
Features: Low viscosity grade for spray applicationFast dryingProvides strong, flexible bondsResists weathering, water, fuels, oil and plasticizersBonds vinyl extrusions and sheeting (May stain ligh..
Peel Strength 5.26 kN/m

@Temperature 24.0 °C,
Time 432000 sec
30.0 pli

@Temperature 75.2 °F,
Time 120 hour
canvas/canvas
3M Fastbond™ 30H-NF Contact Adhesive
3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M
Peel Strength 5.26 kN/m

@Temperature 24.0 °C,
Time 432000 sec
30.0 pli

@Temperature 75.2 °F,
Time 120 hour
180°, Canvas/Steel
3M Fastbond™ 4213-NF Industrial Adhesive
3M™ Fastbond™ Industrial Adhesive 4213-NF is a white, water dispersed adhesive for bonding many fabrics, supported vinyl, wood, leather and most porous materials. Exhibits outstanding clarity when..
Peel Strength 5.26 kN/m

@Temperature 24.0 °C,
Time 1.81e+6 sec
30.0 pli

@Temperature 75.2 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1099 Nitrile High Performance Plastic Adhesives
Features: It is a medium viscosity grade for most brush or flow applicationsFast dryingProvides strong, flexible bonds.Resists weathering, water, fuels, oil and plasticizers.Bonds vinyl extrusions a..
Peel Strength 5.26 kN/m

@Temperature 24.0 °C,
Time 1.21e+6 sec
30.0 pli

@Temperature 75.2 °F,
Time 336 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1300L Neoprene High Performance Rubber Gasket Adhesives
3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre..