Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.877 kN/m @Temperature -37.0 °C, Time 1.81e+6 sec |
5.00 pli @Temperature -34.6 °F, Time 504 hour |
canvas/canvas |
3M Fastbond™ 30-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Peel Strength | 0.877 kN/m @Temperature -55.0 °C |
5.00 pli @Temperature -67.0 °F |
Aluminum T-Peel; ASTM D1876 |
3M Scotch-Weld™ 183 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flowable product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent e.. |
|||
Peel Strength | 0.877 kN/m @Temperature 23.0 °C |
5.00 pli @Temperature 73.4 °F |
Adhesion on Aluminum; ASTM D3330 |
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Peel Strength | 0.877 kN/m @Temperature 23.0 °C |
5.00 pli @Temperature 73.4 °F |
Adhesion on Aluminum; ASTM D3330 |
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Peel Strength | 0.877 kN/m @Temperature 107 °C |
5.00 pli @Temperature 225 °F |
Adhesion on Aluminum; ASTM D3330 |
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Peel Strength | 0.877 kN/m @Temperature 107 °C |
5.00 pli @Temperature 225 °F |
Adhesion on Aluminum; ASTM D3330 |
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Peel Strength | 0.877 kN/m @Temperature -37.0 °C, Time 1.81e+6 sec |
5.00 pli @Temperature -34.6 °F, Time 504 hour |
canvas/canvas |
3M Fastbond™ 30H-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Peel Strength | 0.877 kN/m @Temperature 82.0 °C, Time 1.81e+6 sec |
5.00 pli @Temperature 180 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 4799 Industrial Adhesive 3M™ Scotch-Weld™ Industrial Adhesive 4799 can be used to bond most EPDM rubber, sponge rubber, rubber sheeting, felt, canvas, linoleum and other lightweight materials to many metals, woods, concre.. |
|||
Peel Strength | 0.877 kN/m @Temperature 66.0 °C |
5.00 pli @Temperature 151 °F |
180°, Canvas/Steel |
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive Features: A light colored, fast drying adhesiveExcellent resistance to aromatic fuels, water and oilUsed to bond many types of plastic films including ABS, cellulose acetate, and PVCInformation prov.. |