Polymer Property : Tensile Strength = 9430 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 65.0 MPa

@Strain 9.00 %,
Temperature 150 °C
9430 psi

@Strain 9.00 %,
Temperature 302 °F
5mm/min
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry)
Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Tensile Strength 65.0 MPa

@Temperature 100 °C
9430 psi

@Temperature 212 °F
ISO 527
BASF Ultradur S 4090 G6 30% Glass Filled PBT
Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicati..
Tensile Strength 65.0 MPa

@Strain 2.00 %,
Temperature 100 °C
9430 psi

@Strain 2.00 %,
Temperature 212 °F
ISO 527
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry)
Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el..