Mechanical Properties Metric English Comments
Tensile Strength 420 MPa

@Diameter 105 - 200 mm
60900 psi

@Diameter 4.13 - 7.87 in
United Cast Bar Unibar 500-7 Continuously Cast Spheroidal Graphite Iron
Offers higher wear resistance, strength & heat-treatment response while still possessing good machinability and excellent surface finishes. Noise and vibration damping are good in this grade.Unibar ..
Tensile Strength 420 MPa

@Diameter 205 - 600 mm
60900 psi

@Diameter 8.07 - 23.6 in
United Cast Bar Unibar 500-7 Continuously Cast Spheroidal Graphite Iron
Offers higher wear resistance, strength & heat-treatment response while still possessing good machinability and excellent surface finishes. Noise and vibration damping are good in this grade.Unibar ..
Tensile Strength 420 MPa

@Thickness 152.4 - 203.2 mm
60900 psi

@Thickness 6.000 - 8.000 in
Typical Strength
Constellium Alumold® 350 Aluminum
Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti..
Tensile Strength 420 MPa

@Thickness 203.2 - 254 mm
60900 psi

@Thickness 8.000 - 10.0 in
Typical Strength
Constellium Alumold® 400 Aluminum
The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds..
Tensile Strength 420 MPa

@Thickness 5.90 - 15.0 mm
60900 psi

@Thickness 0.232 - 0.591 in
Typical Strength
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing ..